Value | Units | Test Method / Conditions | |
Tensile Strength | 66 - 89 | MPa | ASTM D638 |
Hardness | 80 | Shore D | ASTM D2240 |
Elongation at Break | 0.8 - 1.9.0 | % | ASTM D638 |
Tensile Modulus | 9000 - 9700 | Mpa | ASTM D638 |
Flexural Strength | 137 - 157 | MPa | ASTM D790 |
Flexural Modulus | 8700 - 10200 | Mpa | ASTM D790 |
Notched Izod Impact Strength | 14 - 17 | J/m | ASTM D256 |
Poissons Ratio | ~0.32 | - | ASTM D638 |
Penetration Depth (Dp) | 5 | mils | -- |
Critical Exposure (Ec) | 5.9 | mJ/cm2 | -- |
Value | Units | Test Method / Conditions | |
Solid Density | 1.61 | g/cm³ | ASTM D150 |
Viscosity (30°C) | 700 - 1000 | cps | -- |
Liquid Density | 1.6 | g/cm3 | -- |
Value | Units | Test Method / Conditions | |
Coefficient of Thermal Expansion (50-100°C) | 64.2 | ppm/°K | ASTM E 831-93 |
Coefficient of Thermal Expansion (100-150°C) | 81.7 | ppm/°K | ASTM E 831-93 |
Heat Deflection Temperature - HDT (UV Postcure only, 66psi) | 73 | °C | ASTM D648 |
Heat Deflection Temperature - HDT (UV Postcure only, 264 psi) | 62 | °C | ASTM D648 |
Heat Deflection Temperature - HDT (UV + Thermal Postcure (120°C), 66 psi) | 250 | °C | ASTM D648 |
Heat Deflection Temperature - HDT (UV + Thermal Postcure (120°C), 264 psi) | 87 | °C | ASTM D648 |
Value | Units | Test Method / Conditions | |
Dielectric Constant (1 MHz) | 4.2 | - | ASTM D 150 |