Capran® 1000 is a 0.39 mil (10 micron) biaxially oriented nylon 6 is suitable for packaging applications that demand optimum protection and performance. It offers a high gas barrier, excellent toughness and puncture resistance, optical clarity, and exceptional flex crack resistance and optics.
Polymer Name: BOPA (Nylon) Film
Physical Form: Film
Features: Gas Barrier, Good Barrier Properties, Corona Treated, Good Optical Properties, Good Flex Crack Resistance, Excellent Performance
Start Order
SecureOrder Quantity
Price
Available upon quote
Minimum Order Quantity
Quote required
Lead Time
Quote required
Available Incoterms
Quote required
Regional Availability
Quote required
Ask AdvanSix Questions
Ask the Supplier
Popular AdvanSix Products
View All AdvanSix Products Capran® 2500RT
Capran® 1200
Capran® 2500
TypeDocument Name
Brochure
AdvanSix Resins & Films for Packaging
AdvanSix Resins & Films for Packaging
BrochureTechnical Data Sheet
Capran® 1000 Technical Data Sheet
Capran® 1000 Technical Data Sheet
Technical Data SheetKnowde Enhanced TDS
Identification & Functionality
Chemical Family
Polymer Name
Technologies
Product Families
Capran® 1000 Features & Benefits
Applications & Uses
Markets
Plastics & Elastomers Processing Methods
Properties
Physical Form
Typical Properties
Value | Units | Test Method / Conditions | |
Average Thickness Target (at 73°F (22.7°C), 50% RH) | 10 | micron | AdvanSix Method |
Average Thickness Tolerance (at 73°F (22.7°C), 50% RH) | 5 | % | AdvanSix Method |
Coefficient of Friction Kinetic (Film to Film at 73°F (22.7°C), 50% RH) | 0.5 - 0.9 | - | ASTM D-1894 |
Coefficient of Friction Kinetic (Film to Metal at 73°F (22.7°C), 50% RH) | 0.2 - 0.3 | - | ASTM D-1894 |
Dimensional Stability - MD (Hot air at 320°F(160°C), 5 mins) | max. 3 | % | - |
Dimensional Stability - TD (Hot air at 320°F(160°C), 5 mins) | max. 2.5 | % | - |
Elongation at Break - MD (at 73°F (22.7°C), 50% RH) | 80 - 110 | % | ASTM D-882 |
Elongation at Break - TD (at 73°F (22.7°C), 50% RH) | 80 - 110 | % | ASTM D-882 |
Haze (at 73°F (22.7°C), 50% RH) | max. 2 | % | ASTM D-1003 |
Oxygen Transmission Rate (at 77°F/0% RH, 25°C/0% RH) | 60 - 75 | cc/m2 /day | ASTM D-3985 |
Secant Modulus - MD (at 73°F (22.7°C), 50% RH) | 1,724 - 2,413 | MPa | ASTM D-882 |
Secant Modulus - TD (at 73°F (22.7°C), 50% RH) | 1,724 - 2,413 | MPa | ASTM D-882 |
Surface Tension Treated Side (at 73°F (22.7°C), 50% RH) | min. 56 | dynes/cm | ASTM D-2578 |
Surface Tension Untreated Side (at 73°F (22.7°C), 50% RH) | 48 - 54 | dynes/cm | ASTM D-2578 |
Tensile Strength at Break - MD (at 73°F (22.7°C), 50% RH) | 220 - 310 | MPa | ASTM D-882 |
Tensile Strength at Break - TD (at 73°F (22.7°C), 50% RH) | 220 - 310 | MPa | ASTM D-882 |
Water Vapor Transmission Rate (at 100°F/100% RH, 37.7°C/100% RH) | 383 - 434 | gm/m2 /day | ASTM F-1249 |
Yield (at 73°F (22.7°C), 50% RH) | 11.6 | g/sq.m | AdvanSix Method |