Company logo

Delrin® 500CPE NC010

Sold by DuPont
Polymer Name: Polyacetal Homopolymer (POM)
Processing Methods: Injection Molding
Additives Included: Mold Release Agent
Start Order
Secure
Order Quantity
Price
Available upon quote
Minimum Order Quantity
Quote required
Lead Time
Quote required
Available Incoterms
Quote required
Regional Availability
View
Similar Products from DuPont NEW
TypeDocument Name
Brochure
Technology Profile Laser Welding
Technology Profile Laser Welding
Brochure
Other
Hot Runner Manual for Robust Molding of Semi-crystalline Resins
Hot Runner Manual for Robust Molding of Semi-crystalline Resins
Other
Other
DuPont™ Delrin® Drives Productivity and Sustainability for High Speed Filling Lines
DuPont™ Delrin® Drives Productivity and Sustainability for High Speed Filling Lines
Other
Other
Safety Restraint Systems
Safety Restraint Systems
Other
Other
DuPont SVHC Statement - Delrin®, Elvamide®, Minlon®, Rynite®, Vamac®
DuPont SVHC Statement - Delrin®, Elvamide®, Minlon®, Rynite®, Vamac®
Other
Other
Delrin® acetal resin Molding Guide
Delrin® acetal resin Molding Guide
Other
Other
Delrin® vs Acetal Copolymer White Paper
Delrin® vs Acetal Copolymer White Paper
Other
Other
Delrin® Design Guide-Module III
Delrin® Design Guide-Module III
Other
Other
Delrin® 500CPE NC010 Injection Data Sheet
Delrin® 500CPE NC010 Injection Data Sheet
Other
Technical Data Sheet
Delrin® 500CPE NC010 Technical Data Sheet
Delrin® 500CPE NC010 Technical Data Sheet
Technical Data Sheet
Brochure
DuPont Performance Polymers - Self Tapping Screws
DuPont Performance Polymers - Self Tapping Screws
Brochure
Brochure
Electrical/Electronic Thermoplastic Encapsulation
Electrical/Electronic Thermoplastic Encapsulation
Brochure

Knowde Enhanced TDS

Expand All

+

Identification & Functionality

Additives Included
Plastics & Elastomers Functions
Technologies

Delrin® 500CPE NC010 Features & Benefits

Applications & Uses

Processing Notes

Injection Molding

Drying is recommended, but not necessary for newly opened packaging stored in a dry location.

Follow the drying guidelines above in the following cases

  • If moisture is above the Processing Moisture Content recommendation,
  • When a resin container is damaged,
  • When the material is not properly stored in a dry place at room temperature, or

Properties

Physical Form
Part Marking Code
>POM<
Resin ID
POM
Physical Properties
ValueUnitsTest Method / Conditions
Moulding Shrinkage - Normal1.9%ISO 294-4, 2577
Moulding Shrinkage - Parallel2.0%ISO 294-4, 2577
Melt Mass-Flow Rate - MFR (190°C/2.16 kg)15.0g/10minISO 1133
Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Modulus3100.0MPaISO 527-1/-2
Yield Stress72.0MPaISO 527-1/-2
Poisson's Ratio0.37--
Yield Strain18.0%ISO 527-1/-2
Nominal Strain at Break27.0%ISO 527-1/-2
Charpy Impact Strength (23°C)230.0kJ/m²ISO 179/1eU
Charpy Impact Strength (-30°C)230.0kJ/m²ISO 179/1eU
Charpy Notched Impact Strength (23°C)9.0kJ/m²ISO 179/1eA
Charpy Notched Impact Strength (-30°C)8.0kJ/m²ISO 179/1eA
Thermal Properties
ValueUnitsTest Method / Conditions
Melting Temperature (10°C/Min)178.0°CISO 11357-1/-3
Temperature of Deflection Under Load (1.8 Mpa)97.0°CISO 75-1/-2
Other Properties
ValueUnitsTest Method / Conditions
Density1420.0kg/m³ISO 1183
Density of Melt1190.0kg/m³-
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Hold Pressure Range80 - 100MPa-
Drying Temperature80.0°C-
Drying RecommendedYes--
Drying Time (Dehumidified Dryer)2 .0 - 4h-
Mold Temperature Optimum90.0°C-
Min. Mould Temperature80.0°C-
Max. Mould Temperature100.0°C-
Annealing Time - Optional30.0min/mm-
Annealing Temperature160.0°C-
Processing Moisture Content≤ 0.2%-
Melt Temperature Optimum205.0°C-
Min. Melt Temperature200.0°C-
Hold Pressure Time8.0s/mm-
Max. Melt Temperature210.0°C-
Max. Screw Tangential Speed0.3m/s-
VDA Properties
ValueUnitsTest Method / Conditions
Emissionsmax. 2mg/100g/kg/100gVDA 275

Packaging & Availability

Regional Availability

Delrin® 500CPE NC010
DuPont