Delrin® 525GR BK000 is a 25% Glass Reinforced Medium Viscosity Acetal Homopolymer
Polymer Name: Polyacetal Homopolymer (POM)
Processing Methods: Injection Molding
Fillers Included: Glass Fiber
Flexural Modulus: 8500.0 MPa
Start Order
SecureOrder Quantity
Price
Available upon quote
Minimum Order Quantity
Quote required
Lead Time
Quote required
Available Incoterms
Quote required
Regional Availability
View
Popular DuPont Products
View All DuPont Products Delrin® 300TE BK602
Delrin® 500AL NC010
Delrin® 570 NC000
Knowde Enhanced TDS
Identification & Functionality
Fillers Included
Polymer Name
Plastics & Elastomers Functions
Technologies
Product Families
Delrin® 525GR BK000 Features & Benefits
Applications & Uses
Markets
Applications
Plastics & Elastomers End Uses
Plastics & Elastomers Processing Methods
Properties
Mechanical Properties
Value | Units | Test Method / Conditions | |
Tensile Modulus | 9500 | MPa | ISO 527-1/-2 |
Flexural Modulus | 8500 | MPa | ISO 178 |
Poisson's Ratio | 0.34 | - | - |
Stress (at Break) | 150 | MPa | ISO 527-1/-2 |
Strain (at Break) | 3 | % | ISO 527-1/-2 |
Flexural Stress (at 3.5%) | 200 | MPa | ISO 178 |
Charpy Impact Strength (at 23°C) | 50 | kJ/m² | ISO 179/1eU |
Notched Charpy Impact Strength (at 23°C) | 10 | kJ/m² | ISO 179/1eA |
Notched Charpy Impact Strength (at -30°C) | 7.5 | kJ/m² | ISO 179/1eA |
Typical Properties
Value | Units | Test Method / Conditions | |
Resin Identification | POM-GF25 | - | ISO 1043 |
Thermal Properties
Value | Units | Test Method / Conditions | |
Melt Temperature (at 10°C/min) | 178 | °C | ISO 11357-1/-3 |
Temperature of Deflection Under Load (1.8 Mpa) | 172 | °C | ISO 75-1/-2 |
Temperature of Deflection Under Load (0.45 Mpa) | 175 | °C | ISO 75-1/-2 |
Flammability
Value | Units | Test Method / Conditions | |
FMVSS Class | B | - | ISO 3795 (FMVSS 302) |
Burning Rate (at 1mm Thickness) | 44 | mm/min | ISO 3795 (FMVSS 302) |
Other Properties
Value | Units | Test Method / Conditions | |
Density | 1590 | kg/m³ | ISO 1183 |
Processing Information (Injection Molding)
Value | Units | Test Method / Conditions | |
Drying Recommended | yes | - | - |
Drying Temperature | 80 | °C | - |
Drying Time (Dehumidified Dryer) | 2 - 4 | h | - |
Processing Moisture Content | max. 0.2 | % | - |
Hold Pressure Range | 80 - 100 | MPa | - |
Hold Pressure Time | 8 | s/mm | - |
Melt Temperature (Optimum) | 215 | °C | - |
Melt Temperature (Minimum) | 210 | °C | - |
Melt Temperature (Maximum) | 220 | °C | - |
Maximum Screw Tangential Speed | 0.3 | m/s | - |
Mold Temperature (Optimum) | 90 | °C | - |
Mold Temperature (Minimum) | 80 | °C | - |
Mold Temperature (Maximum) | 100 | °C | - |
VDA Properties
Value | Units | Test Method / Conditions | |
Fogging (F-Value, Refraction, Assessed) ᴰˢ | min. 90 | % | ISO 6452 |
Rheological Properties
Value | Units | Test Method / Conditions | |
Melt Mass Flow Rate (at 190°C, 2.16 kg) | 7.5 | g/10min | ISO 1133 |
Mold Shrinkage (Parallel) | 0.4 | % | ISO 294-4, 2577 |
Mold Shrinkage (Normal) | 1.2 | % | ISO 294-4, 2577 |
Note
- [DS]: Derived from similar grade
Regulatory & Compliance
Certifications & Compliance
Packaging & Availability
Country Availability
Regional Availability
Delrin® 525GR BK000
DuPont