TPSiV® 4000-75A SR by DuPont is comprised of Thermoplastic Vulcanizate. It is commonly used It is available in Pellets form.
Polymer Name: Thermoplastic Vulcanizate (TPV)
Processing Methods: Injection Molding, Extrusion
Density: 1100.0 kg/m³
Tear Strength: 64.0 kN/m
Compression Set (70 °C): 70.0 %
Start Order
SecureOrder Quantity
Price
Available upon quote
Minimum Order Quantity
Quote required
Lead Time
Quote required
Available Incoterms
Quote required
Regional Availability
Quote required
Similar Products from DuPont NEW
TypeDocument Name
Other
DuPont ROHS Statement - Molykote®, TPSIV® and MULTIBASE™ Brands
DuPont ROHS Statement - Molykote®, TPSIV® and MULTIBASE™ Brands
OtherTechnical Data Sheet
TPSiV® 4000-75A SR Technical Data Sheet
TPSiV® 4000-75A SR Technical Data Sheet
Technical Data SheetOther
TPSiV® 4000-75A SR Injection Molding Guide
TPSiV® 4000-75A SR Injection Molding Guide
OtherOther
DuPont Smart Home Solutions Smart Speaker by Logitech
DuPont Smart Home Solutions Smart Speaker by Logitech
OtherKnowde Enhanced TDS
Identification & Functionality
Polymer Name
Technologies
TPSiV® 4000-75A SR Features & Benefits
Product Highlights
- Softness
- Silky feel
- Resistance to UV lights
- Resistance to Chemicals
- Outsatnding Colourability
- Can be Recycled and Reused
Applications & Uses
Markets
Applications
Plastics & Elastomers Processing Methods
Use Recommendations
It is a product targeted for soft touch overmoulding on wearable electronics, accessory cases for consumer electronics and flexible pipe connectors in portable water systems.
Processing Notes
Injection molding
TPSiV® elastomers products can be manufactured using standard thermoplastic manufacturing processes, including overmolding or co-molding with plastic substrates such as polycarbonate, ABS and nylons.
TPSiV® elastomers self-adhere to hard plastics to enable unique overmolding options. The extremely silky feel of TPSiV elastomers does not require additional processing or coating steps.
Properties
Compatible Polymers & Resins
Mechanical Properties
Value | Units | Test Method / Conditions | |
Compression Set (at 23°C) | 19.0 | % | ISO 815 |
Hardness (3s) | 77 | Shore A | ISO 7619-1 |
Compression Set (at 70°C) | 70.0 | % | ISO 815 |
Hardness (3 sec) | 77 | Shore A | ISO 7619-1 |
Strain at Break | 600.0 | % | ISO 527-1/-2 |
Stress (at 100% Strain) | 3.9 | MPa | ISO 527-1/-2 |
Stress at Break | 15.8 | MPa | ISO 527-1/-2 |
Tear Strength (Normal) | 64.0 | kN/m | ISO 34-1 |
Physical Properties
Value | Units | Test Method / Conditions | |
Melt Mass Flow Rate - MFR (190°C/10kg) | 26.0 | g/10min | ISO 1133 |
Moulding Shrinkage (Parallel) | 2.0 | % | ISO 294-4, 2577 |
Other Properties
Value | Units | Test Method / Conditions | |
Density | 1100.0 | kg/m³ | ISO 1183 |
Processing Information (Injection Molding)
Value | Units | Test Method / Conditions | |
Drying Recommended | yes | - | - |
Drying Temperature | 85.0 | °C | - |
Drying Time (Dehumidified Dryer) | 2-4 | h | - |
Maximum Mould Temperature | 40.0 | °C | - |
Maximum Screw Tangential Speed | 0.4 | m/s | - |
Melt Temperature Optimum | 190.0 | °C | - |
Minimum Mould Temperature | 20.0 | °C | - |
Mold Temperature Optimum | 30.0 | °C | - |
TPSiV® 4000-75A SR
DuPont