Terratek® BD5100

1 of 39 products in this brand

Polymer Name: Thermoplastic Starch (TPS)

Processing Methods: Injection Molding

Labeling Claims: Bio-based, Biodegradable, Sustainable

Tensile Strength: 35.12522 - 35.12522 MPa, 35.1762 - 35.1762 MPa

Density: 1575.0 - 1575.0 kg/m³

Technical Data Sheet

Similar Products

  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Chemical Family
Fillers Included
Plastics & Elastomers Functions
Technologies

Features & Benefits

Applications & Uses

Plastics & Elastomers Processing Methods
General Processing Recommendations

Terratek® BD5100 resin needs to be dried before processing if the moisture is above 0.1%. Resin will dry quickly at 150°F in a desiccant dryer, in approximately 2 to 4 hours. Avoid prolonged resin exposure to air during molding or storage as the material can pick up moisture.

Typical injection molding temperatures are listed below. These are only a guide and may need to be changed based on the particular application:

Rear 330°F to 350°F
Middle 340°F to 360°F
Front 340°F to 375°F
Nozzle 340°F to 375°F
Mold 60°F to 120°F

The melt temperature of the resin should remain below 400°F to prevent the material from discoloring and having a burnt odor.

Properties

Typical Properties
ValueUnitsTest Method / Conditions
Specific Gravity1.575ASTM D792
Shrinkage0.009in/in
Melt Index (190°C, 2.06kg)35g/10 min
Tensile Strength5098psiASTM D638
Tensile Modulus236000psiASTM D638
Flex Strength9173psiASTM D790
Flex Modulus231133psiASTM D790
Notched Izod1.07ft lb/inASTM D256

Packaging & Availability

Packaging Type
Packaging

Terratek® BD5100 resin is typically packaged in a sealed plastic-lined Gaylord at 1200 lbs/Gaylord.

Storage & Handling

Storing
  • The product should be stored in a cool, dry, and sanitary area to achieve maximum stability.
  • Keep material in a sealed package or container to prevent excess moisture absorption.