Green Dot’s Terratek® FX1515 resin needs to be dried before processing. If resin is in a sealed box, dry resin at 90°F to 100°F for 2 to 3 hours. If resin is in an open box, dry resin at 100°F to 120°F for 4 to 5 hours. For best molding results, larger gates and runners are recommended. The injection pressure required to fill the mold is much higher than typical injection molding grade plastics.
Typical injection molding temperatures are listed below, these are only a guide and may need to be changed based on the particular application :
Rear 300°F to 330°F Middle 300°F to 330°F Front 300°F to 330°F Nozzle 300°F to 330°F Processing at temperatures above 350° F and in combination with high shear conditions such as high injection speed may result in thermal degradation of this resin.
Properties
- Typical Properties
Value | Units | Test Method / Conditions | |
Specific Gravity | 1.22 | — | ASTM D792 |
Shrinkage | 0.003 | in/in | ASTM D955 |
Melt Index (190°C, 2.06kg) | 14 | g/10 min | ASTM D1238 |
Tensile Strength (Break) | 1300 | psi | ASTM D638 |
Tensile Modulus | 7122 | psi | ASTM D638 |
Elongation | 400 | % | — |
Notched Izod | No break | — | ASTM D256 |
Flex Strength | 251.4 | psi | ASTM D790 |
Flex Modulus | 7000 | psi | ASTM D790 |
Hardness | A85 | Shore A | ASTM 2240 |
Regulatory & Compliance
- Certifications & Compliance
Packaging & Availability
- Packaging Type
- Packaging
Terratek® FX1515 resin is typically packaged in a sealed plastic-lined drum of 250 lbs.
Storage & Handling
- Storing