Terratek® SC50 is a proprietary blend of wheat starch and polypropylene for injection molding applications. SC 50 contains 50% wheat starch by weight, however, a range of properties can be achieved by altering the starch to plastic ratio and by the inclusion or admission of other additives. Formulations containing anywhere from 30% to 65% starch are available upon request.

Polymer Name: TPS/PP Alloy

Labeling Claims: Bio-based, Biodegradable, Environmentally Friendly, From Renewable Resources, Sustainable

Processing Methods: Extrusion, Injection Molding, Profile Extrusion

Density: 1096.0 - 1096.0 kg/m³, 1100.0 - 1100.0 kg/m³

Tensile Strength: 28.75886 - 28.75886 MPa, 28.8006 - 28.8006 MPa

    Knowde Enhanced TDS

    Identification & Functionality

    Polymer Name
    Plastics & Elastomers Functions
    Technologies

    Features & Benefits

    Applications & Uses

    Plastics & Elastomers Processing Methods
    General Processing Recommendations

    Due to the hydroscopic nature of the natural fillers in this material, pre-drying the resin may be required.  Green Dot recommends that the moisture level of the resin not be above 0.3% as measured by loss-in-weight at 300¬°F for 15 minutes.  If the moisture is above the recommended level, the resin should be dried in a desiccant dryer at 150°F until the moisture is at or below the recommended level.  Failure to dry the material can cause processing problems normally associated with moisture in plastics. For best molding results, larger gates and runners are recommended. The injection pressure required to fill the mold is much higher than typical injection molding grade plastics.

    Typical injection molding temperatures are listed below, these are a guide and may need to be changed based on the particular application :

    Rear 350°F to 360°F
    Middle 350°F to 360°F
    Front 360°F to 375°F
    Nozzle 360°F to 375°F
    Mold 60°F to 170°F

    The melt temperature of the resin should remain below 400°F to prevent the material from discoloring and having a burnt odor.

    Properties

    Typical Properties
    ValueUnitsTest Method / Conditions
    Melt Index (230°C, 2.16kg)31.1g/10 minASTM D1238
    Tensile Strength4174psiASTM D638
    Tensile Modulus375826psiASTM D638
    Specific Gravity1.096g/cm³ASTM D792
    Shrinkage0.011in/in
    Melt Index (230C 2.16kg)31.1g/10 minASTM D1238
    Flex Strength7893psiASTM D790
    Flex Modulus3,30,592psiASTM D790
    Elongation2.17%
    Notched Izod0.44ft lb/inASTM D256
    Specific Gravity1.096ASTM D792
    Flex Modulus330592psiASTM D790

    Regulatory & Compliance

    Certifications & Compliance

    Technical Details & Test Data

    General Processing Conditions
    • Green Dot’s Terratek® SC50 resin needs to be dried before processing if the moisture is above 0.5%. Resin will dry quickly at 220°F in a desiccant dryer. Avoid prolonged resin exposure to air during molding or storage as the material can pick up moisture.
    • For best molding results, larger gates and runners are recommended. The injection pressure required to fill the mold is much higher than typical injection molding grade plastics. Typical injection molding temperatures are listed below, these are only a guide and may need to be changed based on the particular application:
    Rear 350°F to 360°F
    Middle 350°F to 360°F
    Front 360°F to 375°F
    Nozzle 360°F to 375°F
    Mold 60°F to 170°F
    • The melt temperature of the resin should remain below 400°F to prevent the material from discoloring and having a burnt odor.

    Packaging & Availability

    Packaging Type
    Packaging

    Terratek® SC50 resin is typically packaged in a sealed plastic-lined Gaylord at 1200 lbs/Gaylord.

    Storage & Handling

    Storing

    The product should be stored in a cool, dry, and sanitary area to achieve maximum stability.