Knowde Enhanced TDS
Identification & Functionality
- Additives Included
- Chemical Family
- Polymer Name
- Technologies
- Product Families
Features & Benefits
- Materials Features
- Key Features
- Easily cleaned.
- Graffiti resistant.
- Resists scratches.
- Will not delaminate.
- RoHS & REACH compliant.
- UV stabilized.
- Easily fabricated.
- Will not swell or rot.
- Never needs painting.
- Will not crack or chip.
Applications & Uses
- Applications
- Plastics & Elastomers End Uses
- Plastics & Elastomers Processing Methods
- Recommended Applications
- Pools.
- Signage.
- Advertising.
- Golf Courses.
- Campgrounds.
- Apartment Buildings.
- Parks.
- Churches.
- Ski Slopes.
- Water Parks.
- Condominiums.
- Amusement Parks.
- Marinas.
- Schools.
- Playgrounds.
- Nature Trails.
- Municipalities.
- Sports Complexes.
- Any Outdoor Application which requires UV inhibitors.
Properties
- Physical Form
- Mechanical Properties
- Typical Properties
- Thermal Properties
- Electrical Properties
Value | Units | Test Method / Conditions | |
Tensile Strength at Yield | 27.6 | MPa | ASTM-D638 |
Ultimate Elongation | min. 600 | % | ASTM-D638 |
Tensile Impact Strength | 147 | KJ/m2 | ASTM-D1822 |
Notched Izod Impact Strength | 159 | J/m | ASTM-D256 |
Compressive Stress at Yield | 10.3 | MPa | ASTM-D695 |
ESCR | 45 | hours | ASTM-D1693 |
ESCR | 35 | hours | ASTM-D1693 |
Durometer Hardness | 64 | Shore D | ASTM-D2240 |
Flexural Modulus | 1379 | MPa | ASTM-D790 |
Coefficient of Friction, Static | 0.31 | — | ASTM-D1894 |
Coefficient of Friction, Kinetic | 0.22 | — | ASTM-D1894 |
Value | Units | Test Method / Conditions | |
Density | 0.955 | g/cc | ASTM-D1505 |
Melt Index | 0.25 | g/10 min | ASTM-D1238 |
Value | Units | Test Method / Conditions | |
Coef. Of Linear Thermal Expansion | 1.26 x 10^-4 | cm/cm/°C | ASTM-E831 |
Decomposition Temperature | 345 | °C | Union Carbide |
Vicat Softening Temperature | 125 | °C | ASTM-D1525 |
Heat Deflection Temperature | 77 | °C | ASTM-D648 |
Brittleness Temperature | max. -84 | °C | ASTM-D746 |
Glass Transition Temperature | -125 | °C | Union Carbide |
Continuous Use Temp. | -73 to 82 | °C | — |
Thermal Conductivity | 0.35 | W/m-°K | Private Test |
Burn Rate | 25.4 | mm/min | ASTM-D635 |
Ignition Temperature, Flash Conditions | 341 | °C | ASTM-D1929 |
Ignition Temperature, Self Ignition Conditions | 349 | °C | ASTM-D1929 |
Flame Spread | 98 | — | E84 Tunnel Test |
Smoke Developed | 350 | — | E84 Tunnel Test |
Fire Rating | UL 94 | HB | Underwriters Labs |
Value | Units | Test Method / Conditions | |
Dielectric Constant | 2.35 | — | ASTM-D150 |
Dielectric Strength | 20.1 | KV/mm | ASTM-D149 |
Volume Resistivity | min. 6 x 10^15 | ohm-cm | ASTM-D257 |