LD200-SAHC is designed for applications requiring clarity, strength and stiffness.LD200-SAHC exhibits good processability and clarity. Uses for this resin include, bags, film, packaging.LD200-SAHC meets the requirements of the Food and Drug Administration, 21 CFR Section 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations may apply. Contact your Osterman sales representative for more information.
Polymer Name: Low Density Polyethylene (LDPE)
Processing Methods: Extrusion
Start Order
SecureOrder Quantity
Price
Available upon quote
Minimum Order Quantity
Quote required
Lead Time
Quote required
Available Incoterms
Quote required
Regional Availability
View
Popular Osterman & Company Inc. Products
View all Osterman & Company Inc. ProductsProduct NameProduct FamiliesApplications
Osterlene® LLB100 (-B, -SA, -SAM) Polyolefins
Osterlene® LLB2000-G Polyolefins
Osterlene® LLH500-U Polyolefins
TypeDocument Name
Technical Data Sheet
Osterlene LD200-SAHC Technical Data Sheet
Osterlene LD200-SAHC Technical Data Sheet
Technical Data SheetKnowde Enhanced TDS
Identification & Functionality
Chemical Family
Polymer Name
Plastics & Elastomers Functions
Technologies
Product Families
Osterlene® LD200-SAHC Features & Benefits
Labeling Claims
Applications & Uses
Markets
Plastics & Elastomers End Uses
Plastics & Elastomers Processing Methods
Properties
Physical Properties
Value | Units | Test Method / Conditions | |
Melt Mass-Flow Rate - MFR (190°C/2.16 kg) | 2 | g/10 min | ASTM D1238 |
Density | 0.921 | g/cm3 | ASTM D1505 |
Mechanical Properties
Value | Units | Test Method / Conditions | |
Dart Drop Impact Strength | 90 | g | ASTM D1709 |
Thermal Properties
Value | Units | Test Method / Conditions | |
Vicat Softening Temperature | 201 | °F | ASTM D1525 |
Film Properties
Value | Units | Test Method / Conditions | |
Tensile Strength at Yield - MD | 1500 | psi | ASTM D882 |
Tensile Strength at Yield - TD | 1100 | psi | ASTM D882 |
Tensile Strength at Break - MD | 3800 | psi | ASTM D882 |
Tensile Strength at Break - TD | 3300 | psi | ASTM D882 |
Tensile Elongation at Break - MD | 300 | % | ASTM D882 |
Tensile Elongation at Break - TD | 510 | % | ASTM D882 |
Secant Modulus at 1% Secant - MD | 28000 | psi | ASTM D882 |
Secant Modulus at 1% Secant - TD | 33000 | psi | ASTM D882 |
Elmendorf Tear Strength - MD | 350 | g | ASTM D1922 |
Elmendorf Tear Strength - TD | 200 | g | ASTM D1922 |
Optical Properties
Value | Units | Test Method / Conditions | |
Gloss (45°) | 75 | - | ASTM D2457 |