ROMILOY® 8170 is PC/ASA, injection molding grade, chlorine-, bromine- and antimon-free flame retardant.

Polymer Name: PC/ASA Alloy

Processing Methods: Injection Molding

Density: 1180.0 - 1180.0 kg/m³

Flexural Modulus: 2550.0 - 2550.0 MPa

Technical Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Additives Included
Polymer Name
Plastics & Elastomers Functions
Technologies

Features & Benefits

Materials Features

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Physical Form
Physical Properties
ValueUnitsTest Method / Conditions
Water Absorption (23 °C, 50 % RH, 24 h)0.3%DIN EN ISO 62
Density (23 °C, 50 % RH)1.18g/cm³DIN EN ISO 1133
Mechanical Properties
ValueUnitsTest Method / Conditions
Elongation at Break (50 mm/min 23 °C)min. 15%DIN EN ISO 527
Flexural Modulus (2 mm/min 23 °C)2550MPaDIN EN ISO 178
Flexural Strength (2 mm/min 23 °C)92MPaDIN EN ISO 178
Impact Strength (Charpy)n.b.DIN EN ISO 179/1eU
Notched Impact Strength (Charpy at 80 x 10 x 4 23 °C)24kJ/m²DIN EN ISO 179/1eA
Tensile Modulus (1 mm/min 23 °C)2600MPaDIN EN ISO 527
Tensile Strength (50 mm/min 23 °C)58MPaDIN EN ISO 527
Thermal Properties
ValueUnitsTest Method / Conditions
Flammability (File No.: 148878 → UL listed)V0, 5VBUL94
Glow Wire Flammability Index (GWFI)960°CDIN EN 60695-2-12
Glow Wire Ignition Temperature (GWIT)700°CDIN EN 60695-2-13
Heat deflection temperature (HDT/A)75°CDIN EN ISO 75-1
Melt Mass-Flow Rate (MFR)25g/10 minDIN EN ISO 1133
Processing Shrinkage (220 °C, 10 kg)0.3 0.6%DIN EN ISO 294-4
Vicat Softening Temperature (B 50)101°CDIN EN ISO 306