LNP™ COLORCOMP™ Compound D1000F

1 of 77 products in this brand
SABIC's Specialties Business LNP COLORCOMP D1000F compound is based on unfilled Polycarbonate (PC) resin. Added features of this grade include: Superior Molding. This product does not contain PFAS intentionally added during SHPP’s manufacturing process and are not expected to contain unintentional PFAS impurities. Each user is responsible for evaluating the presence of unintentional PFAS impurities.

Polymer Name: Polycarbonate (PC)

Additives Included: Heat Stabilizer

Processing Methods: Injection Molding

Technical Data Sheet

Knowde Enhanced TDS

Identification & Functionality

Additives Included
Chemical Family
Polymer Name
Plastics & Elastomers Functions
Technologies

Features & Benefits

Labeling Claims

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Color
Flame Rating
Physical Properties
ValueUnitsTest Method / Conditions
Density ¹¹1.19g/cm³ASTM D792
Melt Flow Rate (at 300°C, 1.2 kgf) ¹¹17.5g/10 minASTM D1238
Mold Shrinkage (flow, 3.2 mm) ᵍ ¹¹0.5 - 0.7%SABIC method
Specific Gravity ¹¹1.2ASTM D792
Specific Volume ¹¹0.83cm³/gASTM D792
Water Absorption (at 23°C, 24hrs) ¹¹0.15%ASTM D570
Water Absorption (at 23°C, saturated) ¹¹0.35%ASTM D570
Water Absorption (Equilibrium, at 100°C) ¹¹0.58%ASTM D570
Mechanical Properties
ValueUnitsTest Method / Conditions
Flexural Modulus (at 1.3 mm/min, 50 mm span) ¹¹2340MPaASTM D790
Flexural Stress (Yield, 1.3 mm/min, 50 mm span) ¹¹96MPaASTM D790
Hardness (Rockwell M) ¹¹70ASTM D785
Hardness (Rockwell R) ¹¹118ASTM D785
Taber Abrasion (CS-17, 1 kg) ¹¹10mg/1000cyASTM D1044
Tensile Strain (Break, Type I, 50 mm/min) ¹¹125%ASTM D638
Tensile Strain (Yield, Type I, 50 mm/min) ¹¹7%ASTM D638
Tensile Stress (Break, Type I, 50 mm/min) ¹¹68MPaASTM D638
Tensile Stress (Yield, Type I, 50 mm/min) ¹¹62MPaASTM D638
Thermal Properties
ValueUnitsTest Method / Conditions
Coefficient of Thermal Expansion (at -40°C to 95°C, flow) ¹¹0.00006841/°CASTM E831
Heat Deflection Temperature (at 0.45 MPa, 6.4 mm, Unannealed) ¹¹137°CASTM D648
Heat Deflection Temperature (at 1.82 MPa, 6.4 mm, Unannealed) ¹¹129°CASTM D648
Relative Temperature Index (Electrical) ᵖ ¹¹130°CUL 746B
Relative Temperature Index (Mechanical with impact) ᵖ ¹¹130°CUL 746B
Relative Temperature Index (Mechanical without impact) ᵖ ¹¹130°CUL 746B
Specific Heat ¹¹1.25J/g-°CASTM C351
Thermal Conductivity ¹¹0.25W/m-°CASTM C177
Vicat Softening Temperature (Rate B/50) ¹¹154°CASTM D1525
Electrical Properties
ValueUnitsTest Method / Conditions
Comparative Tracking Index (UL, PLC) ¹¹2PLC CodeUL 746A
Dielectric Strength (in air, at 3.2mm) ¹¹14.9kV/mmASTM D149
Dissipation Factor (at 50/60 Hz) ¹¹0.0009ASTM D150
Dissipation Factor (at at 1 MHz) ¹¹0.01ASTM D150
High Ampere Arc Ignition (PLC 0) ¹¹min. 1.5mmUL 746A
High Ampere Arc Ignition (PLC 1) ¹¹min. 3mmUL 746A
High Ampere Arc Ignition (PLC 2) ¹¹min. 1.1mmUL 746A
High Voltage Arc Track Rate (PLC) ¹¹2PLC CodeUL 746A
Hot Wire Ignition (PLC 2) ¹¹min. 1.5mmUL 746A
Hot Wire Ignition (PLC 3) ¹¹min. 1.1mmUL 746A
Relative Permittivity (1 MHz) ¹¹2.96ASTM D150
Relative Permittivity (50/60 Hz) ¹¹3.17ASTM D150
Volume Resistivity ¹¹max. 1E+17Ω.cmASTM D257
Optical Properties
ValueUnitsTest Method / Conditions
Haze (at 2.54 mm) ¹¹1%ASTM D1003
Light Transmission (at 2.54 mm) ¹¹88%ASTM D1003
Refractive Index ¹¹1.586ASTM D542
Impact Properties
ValueUnitsTest Method / Conditions
Falling Dart Impact (at 23°C) ¹¹169JASTM D3029
Instrumented Dart Impact Energy (Peak, at 23°C) ¹¹62JASTM D3763
Izod Impact (Notched, at 23°C) ¹¹694J/mASTM D256
Izod Impact (Unnotched, at 23°C) ¹¹3204J/mASTM D4812
Tensile Impact Strength (Type S) ¹¹546kJ/m²ASTM D1822
Injection Molding
ValueUnitsTest Method / Conditions
Drying Temperature ⁷120°C
Drying Time ⁷3 - 4Hrs
Drying Time (Cumulative) ⁷48Hrs
Maximum Moisture Content ⁷0.02%
Melt Temperature ⁷280 - 305°C
Nozzle Temperature ⁷275 - 300°C
Front - Zone 3 Temperature ⁷280 - 305°C
Middle - Zone 2 Temperature ⁷270 - 295°C
Rear - Zone 1 Temperature ⁷260 - 280°C
Mold Temperature ⁷70 - 95°C
Back Pressure ⁷0.3 - 0.7MPa
Screw Speed ⁷40 - 70rpm
Shot to Cylinder Size ⁷40 - 60%
Vent Depth ⁷0.025-0.076mm
Flame Characteristics
ValueUnitsTest Method / Conditions
UL Recognized (94HB Flame Class Rating) ᵖmin. 0.7mmUL 94
UV-light (Water exposure/immersion) ᵖF2UL 746C
Note
  • ᵍ Measurements made from Laboratory test Coupon. Actual shrinkage may vary outside of range due to differences in processing conditions, equipment, part geometry and tool design. It is recommended that mold shrinkage studies be performed with surrogate or legacy tooling prior to cutting tools for new molded article.
  • ᵖ UL ratings shown on the technical datasheet might not cover the full range of thicknesses and colors. For details, please see the UL Yellow Card.
  • ⁷ Injection Molding parameters are only mentioned as general guidelines. These may not apply or may need adjustment in specific situations such as low shot sizes, large part molding, thin wall molding and gas-assist molding.
  • ¹¹ The information stated on Technical Datasheets should be used as indicative only for material selection purposes and not be utilized as specification or used for part or tool design.
 

Regulatory & Compliance

Certifications & Compliance

Packaging & Availability

Regional Availability
  • Americas
  • Asia
  • Europe
  • North America