NORYL™ Resin PX9406K

1 of 145 products in this brand
SABIC's Specialties Business NORYL™ PX9406K resin is a non-reinforced blend of polyphenylene ether (PPE) + polystyrene (PS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of 5VB at 2mm, 5VA at 2.5mm and V0 at 1.5mm. NORYL™ PX9406 offers strong electrical performance at thin wall, high heat resistance, low warpage, low moisture absorption, and dimensional stability. This material is an excellent candidate consumer electronics applications.

Polymer Name: PPO/PS Alloy

Processing Methods: Injection Molding

Density: 1100.0 - 1100.0 kg/m³

Flexural Modulus: 2420.0 - 2420.0 MPa

Technical Data Sheet

Knowde Enhanced TDS

Identification & Functionality

Additives Included
Polymer Name
Plastics & Elastomers Functions
Technologies

Features & Benefits

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Stress (Yield, Type I, 50 mm/min) ¹¹66MPaASTM D638
Tensile Stress (Break, Type I, 50 mm/min) ¹¹50MPaASTM D638
Tensile Strain (Yield, Type I, 50 mm/min) ¹¹5.7%ASTM D638
Tensile Strain (Break, Type I, 50 mm/min) ¹¹45%ASTM D638
Tensile Modulus (at 50 mm/min) ¹¹2700MPaASTM D638
Flexural Stress (Yield, at 6.4 mm) ¹¹101MPaASTM D790
Flexural Stress (Yield, 1.3 mm/min, 50 mm span) ¹¹100MPaASTM D790
Flexural Modulus (at 1.3 mm/min, 50 mm span) ¹¹2650MPaASTM D790
Flexural Modulus (at 6.4 mm) ¹¹2650MPaASTM D790
Tensile Stress (Yield, 50 mm/min) ¹¹67MPaISO 527
Tensile Stress (Break, 50 mm/min) ¹¹52MPaISO 527
Tensile Strain (Yield, 50 mm/min) ¹¹5%ISO 527
Tensile Strain (Break, 50 mm/min) ¹¹55%ISO 527
Tensile Modulus (at 1 mm/min) ¹¹2550MPaISO 527
Flexural Stress (Yield, at 2 mm/min) ¹¹104MPaISO 178
Flexural Modulus (at 2 mm/min) ¹¹2420MPaISO 178
Physical Properties
ValueUnitsTest Method / Conditions
Specific Gravity ¹¹1.1ASTM D792
Density ¹¹1.1g/cm³ISO 1183
Melt Volume Rate (at 250°C, 10.0 kg) ¹¹7cm³/10 minISO 1133
Melt Volume Rate (at 280°C, 5.0 kg) ¹¹11cm³/10 minISO 1133
Melt Viscosity (at 250°C, 1500 sec⁻¹) ¹¹525Pa-sISO 11443
Melt Viscosity (at 260°C, 1500 sec⁻¹) ¹¹390Pa-sISO 11443
Melt Viscosity (at 280°C, 1500 sec⁻¹) ¹¹250Pa-sISO 11443
Thermal Properties
ValueUnitsTest Method / Conditions
Heat Deflection Temperature (at 0.45 MPa, 3.2 mm, Unannealed) ¹¹128°CASTM D648
Heat Deflection Temperature (at 1.82 MPa, 3.2mm, Unannealed) ¹¹113°CASTM D648
Heat Deflection Temperature (at 0.45 MPa, 6.4 mm, Unannealed) ¹¹130°CASTM D648
Heat Deflection Temperature (at 1.82 MPa, 6.4 mm, Unannealed) ¹¹121°CASTM D648
Ball Pressure Test (at 123°C to 127°C) ¹¹PassIEC 60695-10-2
Vicat Softening Temperature (Rate A/120) ¹¹144°CISO 306
Vicat Softening Temperature (Rate B/120) ¹¹134°CISO 306
Heat Deflection Temperature/Af (at 1.8 Mpa, Flatw 80*10*4, sp=64mm) ¹¹111°CISO 75/Af
Relative Temperature Index (Electrical) ᵖ ¹¹110°CUL 746B
Relative Temperature Index (Mechanical with impact) ᵖ ¹¹105°CUL 746B
Relative Temperature Index (Mechanical without impact) ᵖ ¹¹110°CUL 746B
Electrical Properties
ValueUnitsTest Method / Conditions
Volume Resistivity ¹¹1.40E+17Ω.cmASTM D257
Dielectric Strength (in air, at 3.2mm) ¹¹49kV/mmASTM D149
High Voltage Arc Track Rate (PLC) ¹¹3PLC CodeUL 746A
Comparative Tracking Index ʳ ¹¹250VIEC 60112
Comparative Tracking Index (UL, PLC) ¹¹2PLC CodeUL 746A
High Ampere Arc Ignition (PLC 0) ¹¹min. 1.5mmUL 746A
Hot Wire Ignition (PLC 0) ¹¹min. 1.5mmUL 746A
Arc Resistance (Tungsten, PLC) ¹¹6PLC CodeASTM D495
Impact Properties
ValueUnitsTest Method / Conditions
Izod Impact (Notched, at 23°C) ¹¹170J/mASTM D256
Izod Impact (Notched, at -30°C) ¹¹100J/mASTM D256
Instrumented Dart Impact Total Energy (at 23°C) ¹¹55JASTM D3763
Izod Impact (Notched, 80*10*4, at 23°C) ¹¹12kJ/m²ISO 180/1A
Izod Impact (Notched, 80*10*4, at -30°C) ¹¹5kJ/m²ISO 180/1A
Charpy Impact (at 23°C, V-notch Edgew 80*10*4 sp=62mm) ¹¹13kJ/m²ISO 179/1eA
Charpy Impact (at -30°C, V-notch Edgew 80*10*4 sp=62mm) ¹¹5kJ/m²ISO 179/1eA
Injection Molding
ValueUnitsTest Method / Conditions
Drying Temperature ⁷105 - 110°C
Drying Time ⁷3 - 4Hrs
Drying Time (Cumulative) ⁷8Hrs
Maximum Moisture Content ⁷0.02%
Melt Temperature ⁷275 - 305°C
Nozzle Temperature ⁷275 - 305°C
Front - Zone 3 Temperature ⁷265 - 305°C
Middle - Zone 2 Temperature ⁷255 - 300°C
Rear - Zone 1 Temperature ⁷245 - 295°C
Mold Temperature ⁷70 - 100°C
Back Pressure ⁷0.3 - 0.7MPa
Screw Speed ⁷20 - 100rpm
Shot to Cylinder Size ⁷30 - 70%
Vent Depth ⁷0.038 - 0.051mm
Flame Characteristics
ValueUnitsTest Method / Conditions
UL Recognized (94V-0 Flame Class Rating) ʳmin. 1.5mmUL 94
UL Recognized (94-5VA Flame Class Rating) ʳmin. 2.5mmUL 94
UL Recognized (94-5VB Flame Class Rating) ʳmin. 2mmUL 94
Glow Wire Flammability Index (at 1.5 mm) ʳ960°CIEC 60695-2-12
Glow Wire Flammability Index (at 2 mm) ʳ960°CIEC 60695-2-12
Glow Wire Flammability Index (at 3 mm) ʳ960°CIEC 60695-2-12
Glow Wire Ignitability Temperature (at 1.5 mm) ʳ800°CIEC 60695-2-13
Glow Wire Ignitability Temperature (at 2.0 mm) ʳ800°CIEC 60695-2-13
Glow Wire Ignitability Temperature (at 3.0 mm) ʳ800°CIEC 60695-2-13
Note
  • ᵖ UL ratings shown on the technical datasheet might not cover the full range of thicknesses and colors. For details, please see the UL Yellow Card.
  • ʳ UL Ratings shown on the technical datasheet might not cover the full range of thicknesses, colors and regions. For details, please see the UL Yellow Card.
  • ⁷ Injection Molding parameters are only mentioned as general guidelines. These may not apply or may need adjustment in specific situations such as low shot sizes, large part molding, thin wall molding and gas-assist molding.
  • ¹¹ The information stated on Technical Datasheets should be used as indicative only for material selection purposes and not be utilized as specification or used for part or tool design.
 

Regulatory & Compliance

Certifications & Compliance

Packaging & Availability

Country Availability
Regional Availability
  • Asia