Espolex® 3785A

1 of 23 products in this brand
Espolex® 3785A is a TPV known for its excellent colorability and appearance. It demonstrates strong adhesion to polypropylene compounds and polyethylene, processing like a thermoplastic while acting like a rubber.   Applications: Automotive interior (gaskets, grips, etc.) Automotive exterior Gaskets Mats Overmolding Bathroom accessories Boats Floor mats Jet-propelled vehicles Mud flaps Weatherstripping Injection molded parts   Features: High flowability Rubber-like elasticity and feel   Benefits: Recyclable

Polymer Name: Thermoplastic Polyolefin (TPO)

Processing Methods: Injection Molding

Features: Consistent High Quality, Cost Effective, Flexible, Good Adhesion, Good Colorability, Good Surface Appearance, Heat Resistance, High Elasticity, High Performance, Light Weight, Low Density, Pigmentable

Density: 880.0 - 880.0 kg/m³

Knowde Enhanced TDS

Identification & Functionality

Chemical Family
Technologies

Features & Benefits

Labeling Claims

Applications & Uses

Compatible Polymers & Resins
Plastics & Elastomers Processing Methods

Properties

Color
Physical Properties
ValueUnitsTest Method / Conditions
Density0.88g/cm³ISO 1183
Melt Flow Rate (230°C/10Kg)40.0g/10minISO 1133
Compression Set (22 hrs at 70 °C)43.0MPaASTM D395
Tensile Strength (500mm/min)5.0MPaISO 37 Die C
Tensile Elongation (500mm/min)450.0%ISO 37 Die C
Durometer Hardness (Instantaneous)72.0Shore AASTM D2240
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Nozzle Temperature370 - 470°F
Front Zone390 - 470°F
Middle Zone370 - 450°F
Rear Zone350 - 430°F
Mold Temperature70 - 120°F
Injection SpeedFast
Screw RPMSlow
Injection Pressure20% more than actual transfer pressure
Back Pressure50 - 100psi
Pack/Hold Pressure (of Injection Pressure)40 - 80%

Technical Details & Test Data

Test Data
  • Effect of Temperature on Hardness

Remarks:
Test method- ASTM D2240
Test specimen - Injection molded specimen

Espolex® 3785A - Test Data

  • Spiral Flow Characteristics (230°C)

Espolex® 3785A - Test Data - 1

  • Effect of Shear Rate on Viscosity (200°C)

The figure shows the relation between shear rate and viscosity of ESPOLEX TPE Series at 200°C in comparison with other thermoplastic resins and elastomers. Since its viscosity is dependent on shear rate, effective processing control can be achieved through the adjustment of injection pressure and injection speed.

Espolex® 3785A - Test Data - 2

  • Coverage of Hardness and Compression Set Values

Espolex® 3785A - Test Data - 3

 

Tool Design Guidelines
Parameter Value
Wall Thickness (WT) 2 – 4 mm
Gate Type Fan Gate
Gate Thickness (GT) 0.6 – 0.9 x WT
Gate Width (GW) > 2 x GT
Gate Land (GL) < 0.75 mm
Runner Type Round
Sprue “O” Diameter 3.5 x WT
Main-Runner (SR) 2.5 x WT
Secondary-Runner (MR) 1.5 x WT
Draft 3 – 6 ° per side
Inside Radius (IR) WT / 2
Outside Radius (OR) WT + IR
Surface Texture Light Stipple
Surface Coating Nickel / Teflon
Vent Quantity 1 Every Inch
Vent Depth

0.013 – 0.025 mm

Vent Width 5 mm