product
Company logo
product
Hifill® PA6 IM HS L BK
Search in

Producer: 
Techmer PM
Brand: 
Hifill
HiFill® PA6 IM HS L BK is a Polyamide 6 (Nylon 6) product. It can be processed by injection molding and is available in North America.Characteristics include: Flame Rated Heat Stabilizer Impact Modified Impact Resistant Lubricated

Hifill® PA6 IM HS L BK

Producer: 
Techmer PM
Brand: 
Hifill
HiFill® PA6 IM HS L BK is a Polyamide 6 (Nylon 6) product. It can be processed by injection molding and is available in North America.Characteristics include: Flame Rated Heat Stabilizer Impact Modified Impact Resistant Lubricated
Take Action

Experts (1)

Knowde Enhanced TDS

Expand All

+

Identification & Functionality

+

Applications & Uses

+
Plastics & Elastomers Processing Methods

Properties

+
Flame Rating
Physical Form
Physical Properties
ValueUnitsTest Method / Conditions
Density / Specific Gravity1.06g/cm3ASTM D792
Molding Shrinkage - Flow (0.125 in)0.013in/inASTM D955
Water Absorption (24 hr)1.5%ASTM D570
Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Strength at Yield7300psiASTM D638
Tensile Elongation at Break200%ASTM D638
Flexural Strength9500psiASTM D790
Flexural Modulus250000psiASTM D790
Notched Izod Impact Strength (73°F, 0.125 in)16ft.lb/inASTM D256
Rockwell Hardness (R-Scale)105-ASTM D785
Thermal Properties
ValueUnitsTest Method / Conditions
Coefficient of Linear Thermal Expansion - Flow0.000055in/in/°FASTM D696
Deflection Temperature Under Load - DTUL (264 psi, Unannealed)125°FASTM D648
Deflection Temperature Under Load - DTUL (66 psi, Unannealed)330°FASTM D648
Electrical Properties
ValueUnitsTest Method / Conditions
Dielectric Strength - Method A (Short-Time)420V/milASTM D149
Volume Resistivity20000000000000ohm.mASTM D257
Flammability
ValueUnitsTest Method / Conditions
Flame Rating (0.06 in)HB-UL 94
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Drying Temperature180°F
Drying Time2.0 to 4.0hr
Suggested Max Moisture0.1%
Front Temperature490 to 555°F
Middle Temperature490 to 555°F
Rear Temperature490 to 555°F
Processing (Melt) Temperature460 to 530°F
Mold Temperature150 to 180°F
Back Pressure50.0 to 100psi
Screw Speed30 to 60rpm
Flame Rating
UL 94 HB
Color
Colors Available
Physical Form
Pellets

Regulatory & Compliance

+
Certifications & Compliance
Certifications
UL Flame Rated

Packaging & Availability

+