product
Company logo
product
Sarlink® TPE ME-2340B-01 BLK
Search in

Producer: 
Teknor Apex
Brand: 
Sarlink
Sarlink ME-2340B-01 BLK is a general purpose thermoplastic elastomer used in automotive molding applications, including exterior. Sarlink ME-2340B-01 BLK is a low hardness, low density, UV stabilized grade exhibiting superior compression set and chemical resistance.

Sarlink® TPE ME-2340B-01 BLK

Producer: 
Teknor Apex
Brand: 
Sarlink
Sarlink ME-2340B-01 BLK is a general purpose thermoplastic elastomer used in automotive molding applications, including exterior. Sarlink ME-2340B-01 BLK is a low hardness, low density, UV stabilized grade exhibiting superior compression set and chemical resistance.
Take Action

Knowde Enhanced TDS

Expand All

+

Properties

+
Physical Form
Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Elongation at Break - Across Flow8.7-ISO 37
Tensile Elongation at Break - Flow6.7-ASTM D412
Tensile Stress at 100% Strain - Across Flow116psiISO 37
Tensile Stress at Break - Flow493psiISO 37
Tensile Stress at Break - Across Flow783psiISO 37
Tensile Stress at 100% Strain - Flow199psiISO 37
Compression Set (158°F, 22 hr)0.3-ASTM D395
Compression Set (73°F, 22 hr)0.18-ASTM D395
Compression Set (257°F, 70 hr)0.83-ISO 815
Compression Set (194°F, 70 hr)0.55-ISO 815
Shore Hardness (Shore A, sec, Injection Molded)41-ISO 868
Shore Hardness (Shore A, 15 sec, Injection Molded)39-ISO 868
Tear Strength - Flow100lbf/inISO 34-1
Tear Strength - Across Flow87lbf/inASTM D624
Physical Properties
ValueUnitsTest Method / Conditions
Melt Mass Flow Rate - MFR (230°C/2.16 kg)6g/10 minASTM D1238
Density0.92g/cm3ASTM D1505
Aging
ValueUnitsTest Method / Conditions
Change in Tensile Strength in Air at 100% Strain - Across Flow (230°F, 1008 hr)0.11-ISO 188
Change in Tensile Strength in Air at 100% Strain - Flow (257°F, 168 hr)-0.0073-ISO 188
Change in Tensile Strength in Air at 100% Strain - Flow (230°F, 1008 hr)0.037-ISO 188
Change in Tensile Strength in Air at 100% Strain - Across Flow (257°F, 168 hr)0.13-ISO 188
Change in Tensile Strength in Air - Flow (257°F, 168 hr)0.32-ISO 188
Change in Tensile Strength in Air - Flow (230°F, 1008 hr)0.21-ISO 188
Change in Tensile Strength in Air - Across Flow (257°F, 168 hr)0.33-ISO 188
Change in Tensile Strength in Air - Across Flow (230°F, 1008 hr)0.39-ISO 188
Change in Tensile Strain at Break in Air - Across Flow (257°F, 168 hr)0.14-ISO 188
Change in Tensile Strain at Break in Air - Flow (257°F, 168 hr)0.29-ISO 188
Change in Tensile Strain at Break in Air - Flow (230°F, 1008 hr)0.22-ISO 188
Change in Tensile Strain at Break in Air - Across Flow (230°F, 1008 hr)0.15-ISO 188
Change in Shore Hardness in Air (Shore A, 257°F, 168 hr)3.7-ISO 188
Change in Shore Hardness in Air (Shore A, 230°F, 1008 hr)4.2-ISO 188
Fill Analysis
ValueUnitsTest Method / Conditions
Apparent Viscosity (392°F, 206 sec^-1)148Pa.sASTM D3835
Processing Information (Extrusion)
ValueUnitsTest Method / Conditions
Die Temperature400 to 440°F
Cylinder Zone Temperature400 to 440°F
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Rear Temperature420 to 460°F
Middle Temperature420 to 460°F
Front Temperature420 to 460°F
Nozzle Temperature420 to 460°F
Processing (Melt) Temperature420 to 460°F
Mold Temperature60 to 90°C
Injection Pressure200 to 1000psi
Screw Speed50 to 120rpm
Back Pressure25.0 to 125psi
Injection RateFast-
Cushion0.150 to 1.00in
Color
Black
Physical Form
Pellets

Regulatory & Compliance

+
Certifications & Compliance
Certifications
RoHS Compliant

Packaging & Availability

+