Knowde Enhanced TDS
Identification & Functionality
- Chemical Family
- Polymer Name
- Plastics & Elastomers Functions
- Technologies
Features & Benefits
- Labeling Claims
- Materials Features
- Features
- It has a high crystallization speed and mechanical strength.
- Trays made with PLASTIVERD HOT plus nucleating additives can resist up to 220oC in conventional ovens and microwaves.
- This thermal resistance allows trays to be taken directly from the freezer and heated in a microwave oven.
Applications & Uses
- Applications
- Plastics & Elastomers End Uses
Properties
- Typical Properties
Value | Units | Test Method / Conditions | |
Intrinsic Viscosity | 0’96 ± 0’02 | dL/gr | ISO 1628 |
Specific Density (Crystalline) | min. 1.40 | g/cm³ | - |
Colour L | min. 85 | - | ASTM 6290 |
Colour b* | max. 0 | - | ASTM 6290 |
Color b | max. 0 | - | ASTM 6290 |
Acetaldehyde | max. 1 | ppm | ASTM F2013 |
Color L | min. 85 | - | ASTM 6290 |
Crystallinity | min. 55 | % | - |
Moisture | max. 0’2 | % | - |
Bulk Density | 840 | kg/m³ | - |
Weight of 20 chips | 320 | mg | - |
Melting Point | 245-255 | ºC | - |
Typical Moulding Temperature | 280-290 | ºC | - |
Drying Conditions - Temperature | 165-175 | ºC | - |
Drying Conditions - Time | 5-6 | h | - |
Regulatory & Compliance
- Certifications & Compliance
- Compliance
- PLASTIVERD HOT complies with the composition of requirements of the Regulation (EC) No 10/2011
- EU directive on Packaging Waste (94/62/EC) and its amendments.