Knowde Enhanced TDS
Identification & Functionality
- Product Type
- Technologies
- Product Families
Features & Benefits
- Labeling Claims
- Ready-to-Use Product Features
- Features
- Applied via dip-spin or spray application methods
- Friction modifiers are integrated into topcoat, resulting in repeatable torque tension characteristics during assembly.
Applications & Uses
- Markets
- Application Area
- Application Method
Properties
- Performance Properties
Value | Units | Test Method / Conditions | |
Coating Thickness (Over 8 micron Basecoat) | min. 5 | microns | - |
Cyclic Corrosion Resistance (Honda Class 1) | 40.0 | Cycles | - |
Cyclic Corrosion Resistance (Honda Class 2) | 60.0 | Cycles | - |
Cyclic Corrosion Resistance (Toyota) | 30.0 | Cycles | - |
Salt Spray | 1500.0 | hours | ATSMB117 |