Uteksol Company Logo

Solplast™ TH 55A8014 A0

1 of 994 products in this brand

Polymer Name: Styrenic Thermoplastic Elastomer

Processing Methods: Injection Molding

Tear Strength: 28.0 - 28.0 kN/m

Strain at Break: 750.0 - 750.0 %

Compression Set (70 °C): 88.0 - 88.0 %

    Knowde Enhanced TDS

    Identification & Functionality

    Chemical Family
    Technologies

    Applications & Uses

    Plastics & Elastomers Processing Methods

    Properties

    Mechanical Properties
    ValueUnitsTest Method / Conditions
    Tensile Strength4.8MPaASTM D 638
    Hardness55Shore AASTM D 2240
    Strain at break750%ISO 527
    Compression set (23°, 24h)18%ISO 815
    Compression set (70°, 24h)88%ISO 815
    Tear Strength28kN/mASTM D1004
    Physical Properties
    ValueUnitsTest Method / Conditions
    Melt Flow Index - MFI (190°C/5 kg)40g/10 minISO 1133
    Density970kg/m3ISO 1183

    Packaging & Availability

    Regional Availability
    • Europe