Magna-Tac™ M773 A/B is a low mixed viscosity, high strength, 100% reactive, room temperature curing formulated epoxy adhesive.

Product Type: Epoxy Adhesive

Compatible Substrates & Surfaces: Ceramic, Composites, Glass, Metal, Plastics, Wood

Cure Method: Air Dry

Application Method: Spray

Technical Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Product Type

Features & Benefits

Ready-to-Use Product Features

Applications & Uses

Application Method
Compatible Substrates & Surfaces
Cure Method
Uses

Magna-Tac M773 is used for:

  • Bonding rigid expanded plastic foams to themselves or to metal, plywood, or other rigid materials;
  • Bonding a wide variety of skins to cores (expanded polystyrene foam, foamed glass, honeycomb, etc.) in the fabrication of sandwich panels.
  • Bonding all metals and other rigid materials (such as glass, ceramics, most plastics, plastic foams, structural laminates) to themselves and to each other.

Note - Fully cured panels consisting of degreased steel or etched aluminum skins and foamed glass cores produced with this adhesive pass FPL Test Cycles (ASTM Test D1037-55T), also given in ASTM C481, Cycle A.

  Mixing Ratio (by weight) Properties Pot Life at 77°F

Aver. Tensile Strength

Part A
Part B
100 PARTS
100 PARTS
For best balance
of properties.
2-3 hours
(1 qt)
2200 psi
Application

Surface Preparation

All bonding surfaces must be thoroughly cleaned, degreased and dried. For plastic surfaces, remove mold release if any.

Preparation of Adhesive

Always stir each part thoroughly first. Proportion accurately and mix slowly to avoid entrapping air. Magna-Tac M773 Part A is colored red; Part B is colored Amber. Mix equal amounts (by volume) and stir until the color of the mixture is uniform. Note: Pot life can be lengthened substantially if shallow mixing vessels are used or smaller batches are mixed. Cover mixed material to prevent water absorption. Mixed adhesive may be applied with paint roller, brush or conventional spray equipment, etc. Apply enough mixed adhesive to leave about 4-6 mils in the final glue line. This may be accomplished by coating 4-6 mils on one surface only or by coating 2-3 mils on each surface. If one surface is porous, more adhesive must be applied to fill the voids and yet produce a final glue line thickness of 4-6 mils.

Mix Ratio

Magna-Tac M773 Part A - 100 parts Magna-Tac M773 Part B - 100 parts.

Curing Information

Cure Time

Room Temperature At room temperature, assemblies can be handled in approximately 8-14 hours. Magna-Tac M773 develops 85% of its maximum strength in 24-48 hours. NOTE: The bond continues to advance in strength for approximately one week.

Typical lap shear values obtained when Magna-Tac 666 is used to bond 0.064" etched 2024T3 aluminum alloy to itself in a 1/2 overlap are as follows:

Test Temperature

Tensile Shear, psi

-67°F 2000
77°F 2500
180°F 400

Fast Cure

If a faster cure is required, the following cycles may be used:

Elevated Temperatures

Temperature Cure Time
150°F 120 minutes
200°F 45 minutes
250°F 30 minutes
300°F 10 minutes

Bonds will continue to improve in strength at room temperature until optimum is reached, usually within 3- 4 days.

Materials It Protects

Bonding rigid expanded plastic foams to themselves or to metal, plywood, or other rigid materials; Bonding a wide variety of skins to cores (expanded polystyrene foam, foamed glass, honeycomb, etc.) in the fabrication of sandwich panels. Bonding all metals and other rigid materials (such as glass, ceramics, most plastics, plastic foams, structural laminates) to themselves and to each other.

Base

Modified epoxy

Properties

Diluent
Do not dilute
Typical Properties
ValueUnitsTest Method / Conditions
Glass Transition (Tg)57.07°C
Hardness60 - 70Shore D
Dielectric Constant (105 cps)2085 - 3.65
Volume Resistivity (22 - 28 °C)Min 1.00 x 10¹²ohm-cm
Thermal Coefficient of Expansion65 x 10⁻⁶inches/inches/°C
Viscosity (77°F, Part B)1000cps
Viscosity (77°F, Part A)20,000cps
Weight Per Gallon (Part A)9.5lbs
Weight Per Gallon (Part B)8.2lbs
Strength2200.0psi
Pot Life (1 quart)45.0minutes
Composition
ValueUnitsTest Method / Conditions
Solid Content (Part A)97.0%
Solid Content (Part B)100.0%

Regulatory & Compliance

Certifications & Compliance

Packaging & Availability

Packaging Type
Container Sizes
  • 1 quart cans
  • 1 gallon cans
  • 5 gallon pails
  • 55 gallon drums

Storage & Handling

Shelf Life
1 year