Cast-Coat Inc. CC3-402A

Cast-Coat Inc. CC3-402A is a general purpose, fire retardant epoxy potting resin exhibiting low abrasion resistance. It is designed to be used where low viscosity and good wetting-out properties are important. Low shrinkage and good thermal shock resistance minimize stress on potted components. A choice of hardeners enable the CC3-402A to be cured either at room temperature or with heat. Even though the entire CC3-402A series offers a low percent of filler separation, it is advisable to always mix the contents in the shipping container prior to use.

Product Type: Potting Compound

Cure Method: Air Dry, Heat Cure

Technical Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Product Type

Features & Benefits

Applications & Uses

Choice of Hardeners
  • H-1 Hardener: Rigid, good dimensional stability, fast cure.
  • H-18 Hardener: Resilient, excellent mechanical and thermal shock, low viscosity, good air release, fast cure.
  • H-10LV Hardener: Variable hardness, excellent impact properties, long pot life
HARDENER PARTS BY WEIGHT PER 100 PARTS OF RESIN POT LIFE 100 GRAM 25°C (77°F) CURE TIME 25°C (77°F) CURE TIME 65°C (149°F)

CURE TIME 125°C (257°F)

H-1 Hardener 7 1 hr. 24 hrs. 2 hrs. - - -
H-18 Hardener 14.5 2 hrs. 24 hrs. 2 hrs. - - -
H-10LV Hardener 20 (rigid) 3 hrs. 24 hrs. 3 hrs. - - -
H-10LV Hardener 43 (semi-flex) 3 hrs. 24 hrs. 3 hrs. - - -
H-10LV Hardener 65 (flexible) 3 hrs. 24 hrs. 3 hrs. - - -
Room Temperature Cure
  • H-1 Hardener: Cures overnight at room temperature or 2 hrs at 65°C. Do not heat cure if the mass exceeds 200 grams.
  • H-18 Hardener: Cures overnight at room temperature or 2 hrs at 65°C. Do not heat cure if the mass exceeds 200 grams.
  • H-10LV Hardener: Cures overnight at room temperature or 3 hrs at 65°C. Do not heat cure if the mass exceeds 300 grams.
Mixing Instructions

Mix CC3-402 thoroughly in it’s shipping container to insure a uniform consistency. Weigh out the desired amount of resin in a clean container. Add the hardener accurately by weight in the proper proportion as specified above. (ie. 7.0 grams of H-1 Hardener and 100 grams of CC3-402A for a total mix of 107.0 grams) Mix thoroughly. Use in a well ventilated area and avoid contact with eyes and skin.

Properties

Flame Rating
Physical & Electrical Properties
ValueUnitsTest Method / Conditions
Coefficient of Thermal Expansion31 x 10^(-6)in/in/’C
Compressive Strength (25°C)22700.0psi
Dielectric Constant (25°C, 100 KC)4.2
Dielectric Strength450.0volts/mil
Dissapation Factor (25°C, 100 KC)0.02
Glass Transistion Temperature (Tg)125.0°C
Heat Distortion65.0°C
Izod Impact (of Notch)0.8ft lbs/in
Linear Shrinkage0.004in/in
Service Temperature (Continuous)-55 - 155°C
Specific Gravity (Catalyzed, 25°C)1.4
Specific Gravity (Uncatalyzed, 25°C)1.5
Tensile Strength (25°C)7200.0psi
Thermal Conductivity1.12W/mK
Viscosity (Catalyzed, 22.5°C)1050.0cps
Viscosity (Uncatalyzed, 22.5°C)13300.0cps
Volume Resistivity (25°C)1016.0ohm-cm
Water Absorption (7 days, 25°C)0.2%