Knowde Enhanced TDS
Identification & Functionality
- Product Type
- Technologies
- Product Families
Features & Benefits
- Labeling Claims
- Ready-to-Use Product Features
- Advantages
- High viscosity and good adhesion.
- Contains both polar and E.P. load bearing additives.
- Reduced friction, prevents scuffing and wear.
- Does not contain any lead type additives.
- Does not contain any harmful solvents.
- Can be applied by lubrication from open bath, drip or pressure feed.
Applications & Uses
- Applications
- Application Area
- Applications
Alpha OG 1500 is suitable for use in a wide range of heavy duty gears and roller applications.
- Heavily loaded open gears.
- Roller bearings.
- Heavily loaded slow moving sliding surfaces.
Properties
- Appearance
- Clear Dark Brown Viscous
- Typical Properties
Value | Units | Test Method / Conditions | |
Density (30°C / 86°F) | 945.0 | kg/m³ | ASTM D4052 |
Kinematic Viscosity (40°C / 104°F) | 1500.0 | mm²/s | ISO 3104 |
Pour Point | -3 (27) | °C(°F) | ASTM D97 |
Flash Point - Closed Cup Method | min. 220 (428) | °C(°F) | ASTM D93 |
Fire Point | min. 230 (446) | °C(°F) | ASTM D92 |
AGMA Grade No. | 9EP | - | - |
Foam Sequence I (Tendency / Stability) | 20.0 | ml | ASTM D892 |
Foam Sequence II (Tendency / Stability) | 20.0 | ml | ISO 6247 |
Foam Sequence III (Tendency / Stability) | 20.0 | ml | ISO 6247 |
Air Release (75°C / 167°F) | 40.0 | min | ASTM D3427 |
Demulsification - Steam method | 1400.0 | sec | IP 19 |
Acid Number | 0.15 | mgKOH/g | ASTM D664 |
Copper Corrosion (3 hrs at 100°C/212°F ) | 1b | - | ASTM D130 |
Timken Ok Load Test | 65 (143) | kg/lb | ASTM D2782 |
FZG Gear Scuffing Test (A/8.3/90) | min. 12 | - | ISO 14635-1 |
Four Ball Wear Test - Wear Scar Diameter (1 hr, 20kg, 1800 rpm) | 0.321 | mm | IP 239 |
Four Ball Wear Test - Initial Seizure Load | 145.0 | kg | IP 239 |
Four Ball Wear Test - Weld Point | 450.0 | kg | IP 239 |