Knowde Enhanced TDS
Identification & Functionality
- Chemical Family
- Composite Materials Functions
- Technologies
Features & Benefits
- Materials Features
Applications & Uses
- Applications
- Composites Processing Methods
Properties
- Physical Form
- Typical Properties
Value | Units | Test Method / Conditions | |
Impact Strength as molded | 2.5 - 3.0 | ft-lb/in | D 256 |
Impact Strength postcured 16 hrs at 475 °F | 1.7 | ft-lb/in | D 256 |
Impact Strength as molded then 8 hrs at 510 °F | 0.96 | ft-lb/in | D 256 |
Impact Strength as molded then postcured 2 hrs at 800 °F | 0.96 | ft-lb/in | D 256 |
Flexural Strength as molded | 7000 - 12000 | psi | D 790 |
Flexural Strength as molded then 8 hrs at 510 °F | 6700 | psi | D 790 |
Flexural Strength as molded then postcured 2 hrs at 800 °F | 3400 | psi | D 790 |
Heat Deflection Temperature postcured at 475 °F | min. 600 | °F | D 648 |
Molding Pressure | 1000 - 2000 | psi | — |
Molding Temperature | 285 - 350 | °F | — |
Mold Shrinkage | 0.000 - 0.0015 | in/in | D 955 |
Specific gravity | 2.15 | — | D 792 |
Flammability (at 1/32") | V-0 | — | — |
Barcol Hardness | 51 - 61 | — | — |
Arc Resistance | min. 255 | Seconds | D 495 |
Arc Resistance then postcured 10 days at 660 °F | min. 300 | Seconds | D 495 |
Dielectric Strength | min. 400 | v/mil | D 149 |