Dhara Petrochemicals Dpnor GF-M-212 is mPPE Black Compounds, reinforced with 20% of glass fiber, for injection molding. Dpnor GF-M-212 is widely used for submersible pump parts like bowls, impellers & diffusers, automotive parts.

Polymer Name: Polyphenylene Ether (PPE)

Processing Methods: Injection Molding

Fillers Included: Glass Fiber

Flexural Modulus: 7453.02 - 7453.02 MPa

  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Fillers Included
Plastics & Elastomers Functions
Technologies

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Flame Rating
Mechanical Properties
ValueUnitsTest Method / Conditions
Izod Impact Strength (Notched) at 23 °C12kg . cm/cmASTM D-256
Abrasion Resistance (CS-17,1000gms,1000 cycles)0.026gmsASTM D 1044
Flexural Modulus76000kg/cm2ASTM D-790
Flexural Strength1233kg/cm2ASTM D-790
Hardness80Shore DASTM D 2240
Tensile Strength at Yield1038kg/cm2ASTM D-638
Typical Properties
ValueUnitsTest Method / Conditions
Density1.2g/ccASTM D792
Heat Deflection Temperature at 18.5 Kg/cm2130°CASTM D-648
Melt Flow Index at 280 °C /3.8 Kg1.46g/10 minASTM D 1238
Shrinkage (In Flow Direction at3.2 mm Thickness)0.29%ASTM D 955
Water Absorption (24 hrs immersion at 23 +/- 1 °C)0.05%ASTM D 570
Flammability
ValueUnitsTest Method / Conditions
Flammability Rating At 3.2 mm ThicknessHBmm/mm UL 94

Regulatory & Compliance

Certifications & Compliance

Technical Details & Test Data

Processing Parameters

Pre Drying - With a dehumidified air drying equipment at 80~100°C for 2-3 Hours.

Recommended Molding Conditions :
  • Barrel temperatures : 
    • Feed zone : 250-255°C
    • Compression zone : 255-260°C
    • Front zone : 260-265°C
    • Nozzle : 265-270°C
  • Mold temperatures : 80-100°C