Properties
- Flame Rating
- Mechanical Properties
- Typical Properties
- Electrical Properties
- Flammability
Value | Units | Test Method / Conditions | |
Hardness | 78 | Shore D | ASTM D 2240 |
Flexural Modulus | 7500 | MPa | ISO 179 |
Flexural Strength | 128 | MPa | ISO 178 |
Izod Impact Strength (Notched) at 23 °C | 48 | Kj/m 2 | ASTM D-256 |
Nominal Tensile Strain | 10 | % | ISO 527 |
Tensile Strength at Yield | 115 | MPa | ISO 527 |
Value | Units | Test Method / Conditions | |
Density at 25 °C | 1.25 | g/cc | ISO 1183 |
Heat Deflection Temperature at 1.82 MPa | 132 | °C | ASTM D-648 |
Melting Point | 260 | °C | ISO 11357-1/3 |
Moisture Absorption | 0.12 | % | IS0 62 |
Moulding Shrinkage | 0.25 | % | ISO 2577 |
Value | Units | Test Method / Conditions | |
Volume Resistivity | 10^16 | Ohm-cm | IEC 60112 |
Value | Units | Test Method / Conditions | |
Flammability Rating | HB | mm/mm | UL 94 |
Regulatory & Compliance
- Certifications & Compliance
Technical Details & Test Data
- Processing Parameters
Pre Drying - With a dehumidified air drying equipment at 80~100°C for 2-3 Hours.
Recommended Molding Conditions :
- Barrel temperatures :
- Feed zone : 250-255°C
- Compression zone : 255-260°C
- Front zone : 260-265°C
- Nozzle : 265-270°C
- Mold temperatures : 80-100°C
- Barrel temperatures :