Knowde Enhanced TDS
Identification & Functionality
- Additives Included
- Chemical Family
- Fillers Included
- Polymer Name
- Plastics & Elastomers Functions
- Technologies
Features & Benefits
- Materials Features
Applications & Uses
- Applications
- Plastics & Elastomers Processing Methods
- Processing Guidelines
Predrying
The moisture of CompaDur must not exceed 0,02% in order to avoid the degradation of the polymer during processing. Therefore we strongly recommend to pre-dry the product, preferably by air dryer (dry air). The product should be dried over 2 to 4 hours at 120 - 140 ° C.
Properties
- Color
- Flame Rating
- Typical Properties
- Processing Information (Injection Molding)
Value | Units | Test Method / Conditions | |
Density (23°C) | 1.54 | g/m³ | ISO 1183 |
Melt Volume Flow Rate (250/2,16) | 14 | cm³/10 min | ISO 1133 |
Tensile Modulus (1mm/min) | 4200 | mPa | ISO 527 |
Stress at Break (5 mm/min) | 50 | mPa | ISO 527 |
Strain at Break (5 mm/min) | 3 | % | ISO 527 |
Flammability (0,8 mm) | HB | Class | UL 94 |
Value | Units | Test Method / Conditions | |
Cylinder (Temperature) | 250 - 265 | °C | — |
Nozzle (Temperature) | 260 - 270 | °C | — |
Mass (Temperature) | 260 - 270 | °C | — |
Mould (Temperature) | 75 - 100 | °C | — |
Melt Residence Time | min. 5-10 | — | — |
Injection Pressure | 600 - 1000 | bar | — |
Post Pressure | 400 - 800 | bar | — |
Dynamic Pressure | 10 - 30 | bar | — |
Screw Speed | 80 | Upm | — |
Injection Rate | High | — | — |
Nozzle | Open | — | — |
Regulatory & Compliance
- Certifications & Compliance
Packaging & Availability
- Regional Availability