Polymer Name: Acrylonitrile Butadiene Styrene (ABS)

Processing Methods: Profile Extrusion

Melt Flow Index: 1.4 - 1.4 g/10 min

Technical Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Plastics & Elastomers Functions
Technologies

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Flame Rating
Flame Rating
UL 94 HB
Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Strength at Yield39MPaASTM D 638
Rockwell Hardness108Scale RASTM D785
Tensile Elongation at Break4.4-ASTM D412, ISO 37
Flexural Strength58MPaASTM D 790
Flexural Modulus1793MPaASTM D 790
Izod Notched Impact Strength (73°F)641J/mASTM D256
Physical Properties
ValueUnitsTest Method / Conditions
Melt Flow Rate - MFR (200 °C/10.0 kg)13g/10minASTM D1238
Melt Flow Rate - MFR (200°C/5.0 kg)1.4g/10minASTM D1238
Molding Shrinkage - Cross Flow (0.126 in (3.20 mm))0.004 - 0.007mmASTM D955
Molding Shrinkage - Flow (0.126 in (3.20 mm))0.004mmASTM D955
Specific Gravity1.03-ASTM D 792
Thermal Properties
ValueUnitsTest Method / Conditions
Heat Deflection Temperature - HDT (264 psi)97°CASTM D648
Flammability
ValueUnitsTest Method / Conditions
Flame Rating (0.062)HB-UL 94
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Drying Temperature180 - 200°F
Drying Time2.0 - 4.0h
Maximum Drying Time5h
Suggested Maximum Moisture0.001%
Rear Barrel Temperature370 - 450°F
Middle Barrel Temperatures400 - 475°F
Front Barrel Temperatures425 - 500°F
Nozzle Temperature425 - 525°F
Back Pressure25 - 100psi
Mold Temperature90 - 160°F
Screw Speed25 - 75rpm
Melt Temperature425 - 525°F
Additional Information
ValueUnitsTest Method / Conditions
Filler Content0%

Regulatory & Compliance

Certifications & Compliance