company tower banner
EnCom Polymers Company Logo

EnCore™ 2002V

1 of 13 products in this brand

Polymer Name: Acrylonitrile Butadiene Styrene (ABS)

Processing Methods: Injection Molding

Melt Flow Index: 6.0 - 6.0 g/10 min

Technical Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Plastics & Elastomers Functions
Technologies

Features & Benefits

Materials Features

Applications & Uses

Plastics & Elastomers End Uses
Plastics & Elastomers Processing Methods

Properties

Color
Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Strength at Yield34MPaASTM D 638
Tensile Elongation at Break4.4-ASTM D412, ISO 37
Tensile Modulus1931MPaASTM D 638
Flexural Strength41MPaASTM D 790
Flexural Modulus2000MPaASTM D 790
Izod Notched Impact Strength (73°F)107J/mASTM D256
Physical Properties
ValueUnitsTest Method / Conditions
Melt Flow Rate - MFR (220°C/10 kg)6g/10minASTM D1238
Molding Shrinkage - Cross Flow (0.126 in (3.20 mm))0.004 - 0.007mmASTM D955
Molding Shrinkage - Flow (0.126 in (3.20 mm))0.004 - 0.008%ASTM D955
Specific Gravity1.05-ASTM D 792
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Drying Temperature180 - 200°F
Drying Time2.0 - 4.0h
Maximum Drying Time7h
Melt (processing) Temperatures425 - 525 °F
Suggested Maximum Moisture0.1%
Rear Barrel Temperatures370 - 450 °F
Middle Barrel Temperatures400 - 475 °F
Front Barrel Temperatures425 - 500 °F
Nozzle Temperature425 - 525 °F
Back Pressure25 - 100psi
Mold Temperatures120 - 170 °F
Screw speed25 - 75rpm