Polymer Name: Acrylonitrile Butadiene Styrene (ABS)

Processing Methods: Injection Molding, Profile Extrusion

Melt Flow Index: 5.0 - 5.0 g/10 min

Technical Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Plastics & Elastomers Functions
Technologies

Applications & Uses

Plastics & Elastomers End Uses
Plastics & Elastomers Processing Methods

Properties

Flame Rating
Flame Rating
UL 94 HB
Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Strength at Yield45MPaASTM D 638
Tensile Elongation at Break4.4-ASTM D412, ISO 37
Flexural Strength72MPaASTM D 790
Flexural Modulus2393MPaASTM D790
Izod Notched Impact Strength (73°F)320J/mASTM D256
Physical Properties
ValueUnitsTest Method / Conditions
Melt Flow Rate - MFR (230°C/3.8 kg)5g/10minASTM D1238
Molding Shrinkage - Cross Flow (0.126 in (3.20 mm))0.004 - 0.007mmASTM D955
Molding Shrinkage - Flow (0.126 in (3.20 mm))0.004 - 0.008%ASTM D955
Specific Gravity1.04-ASTM D 792
Flame Rating (0.062)HB-UL 94
Flame Rating (0.125)HB-UL 94
Thermal Properties
ValueUnitsTest Method / Conditions
Heat Deflection Temperature - HDT (264 psi)84°CASTM D648
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Drying Temperature180 - 200°F
Drying Time2.0 - 4.0h
Maximum Drying Time7h
Melt (processing) Temperatures425 - 525 °F
Suggested Maximum Moisture0.1%
Rear Barrel Temperatures370 - 450 °F
Middle Barrel Temperatures400 - 475 °F
Front Barrel Temperatures425 - 500 °F
Nozzle Temperature425 - 525 °F
Back Pressure25 - 100psi
Mold Temperatures120 - 170 °F
Screw speed25 - 75rpm