Value | Units | Test Method / Conditions | |
Tensile Strength at Yield | 28 | MPa | ASTM D 638 |
Tensile Elongation at Break | 100 | % | ISO 527 |
Flexural Modulus | 1725 | MPa | ASTM D 790 |
Izod Notched Impact Strength (73°C) | 694 | J/m | ASTM D256 |
Value | Units | Test Method / Conditions | |
Melt Flow Rate - MFR (260°C/3.8 kg) | 5.5 | g/10min | ASTM D1238 |
Molding Shrinkage - Across Flow (0.126 in (3.20 mm)) | 0.406 - 0.508 | mm/mm | ASTM D955 |
Molding Shrinkage - Flow (0.126 in (3.20 mm)) | 0.406 - 0.508 | mm/mm | ASTM D955 |
Specific Gravity | 1.21 | - | ASTM D 792 |
Value | Units | Test Method / Conditions | |
Heat Deflection Temperature - HDT (66 psi) | 150 | °C | ASTM D648 |
Value | Units | Test Method / Conditions | |
Drying Temperature | 93.3 - 104 | °C | — |
Drying Time | 43558 | h | — |
Maximum Drying Time | 8 | h | — |
Suggested Maximum Moisture | 0.04 | % | — |
Rear Barrel Temperature | 238 - 254 | °C | — |
Middle Barrel Temperatures | 243 - 260 | °C | — |
Front Barrel Temperatures | 249 - 266 | °C | — |
Nozzle Temperature | 243 - 266 | °C | — |
Back Pressure | 0.345 - 1.03 | MPa | — |
Mold Temperature | 54.4 - 71.1 | °C | — |
Screw Speed | 30 - 80 | rpm | — |
Vent Depth | 0.013 - 0.0381 | mm | — |
Melt Temperature | 260 - 277 | °C | — |