Value | Units | Test Method / Conditions | |
Tensile Strength at Yield | 54 | MPa | ASTM D 638 |
Tensile Elongation at Break | 7 | - | ASTM D412 |
Tensile Modulus | 2759 | MPa | ASTM D638 |
Flexural Strength | 76 | MPa | ASTM D 790 |
Flexural Modulus | 2414 | MPa | ASTM D 790 |
Izod Notched Impact Strength (73°F) | 112 | J/m | ASTM D256 |
Izod Unnotched Impact Strength | No Break | - | ASTM D256 |
Value | Units | Test Method / Conditions | |
Melt Flow Rate - MFR (190°C/2.16 kg) | 30 | g/10min | ASTM D1238 |
Molding Shrinkage - Flow (0.126 in (3.20 mm)) | 0.508 | mm/mm | ASTM D955 |
Specific Gravity | 1.39 | - | ASTM D 792 |
Value | Units | Test Method / Conditions | |
Coefficient of Linear Thermal Expansion | 1.1e-09 | mm/(mm, °C) | ASTM E831 |
Heat Deflection Temperature - HDT (264 psi) | 95 | °C | ASTM D648 |
Value | Units | Test Method / Conditions | |
Drying Temperature | 170 | °F | — |
Drying Time | 2.0 - 4.0 | h | — |
Suggested Maximum Moisture | 0.0002 | % | — |
Suggested Shot Size | 25 - 33 | % | — |
Rear Barrel Temperature | 340 - 380 | °F | — |
Middle Barrel Temperatures | 360 - 400 | °F | — |
Front Barrel Temperatures | 370 - 420 | °F | — |
Nozzle Temperature | 370 - 420 | °F | — |
Back Pressure | 50 | bar | — |
Mold Temperature | 160 - 200 | °F | — |
Melt Temperature | 360 - 390 | °F | — |