Polymer Name: PC/ABS Alloy

Processing Methods: Injection Molding

Density: 1140.0 - 1140.0 kg/m³

Flexural Modulus: 2317.0 - 2317.0 MPa

Technical Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Polymer Name
Plastics & Elastomers Functions
Technologies

Features & Benefits

Materials Features

Applications & Uses

Plastics & Elastomers End Uses
Plastics & Elastomers Processing Methods

Properties

Flame Rating
Flame Rating
UL 94 HB
Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Strength at Yield54MPaASTM D 638
Tensile Strength at Break54MPaASTM D 638
Tensile Elongation at Break145%ASTM D638
Flexural Strength90MPaASTM D 790
Flexural Modulus2317MPaASTM D790
Izod Notched Impact Strength (-40°C)481J/mASTM D256
Izod Notched Impact Strength (73°F)641J/mASTM D256
Physical Properties
ValueUnitsTest Method / Conditions
Melt Flow Rate - MFR (260°C/5.0 kg)10g/10minASTM D1238
Molding Shrinkage - Flow (0.126 in (3.20 mm))0.178mm/mmASTM D955
Specific Gravity1.14-ASTM D 792
Thermal Properties
ValueUnitsTest Method / Conditions
Heat Deflection Temperature - HDT (264 psi)107°CASTM D648
Heat Deflection Temperature - HDT (66 psi)124°CASTM D648
Flammability
ValueUnitsTest Method / Conditions
Flame Rating (0.125)HB-UL 94
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Drying Temperature180 - 220°F
Drying Time2.0 - 4.0h
Maximum Drying Time4h
Suggested Maximum Moisture0.0002%
Rear Barrel Temperature450 - 500°F
Middle Barrel Temperatures455 - 505°F
Front Barrel Temperatures465 - 525°F
Nozzle Temperature475 - 525°F
Back Pressure25 - 100psi
Mold Temperature175 - 200°F
Screw Speed25 - 75rpm
Melt Temperature475 - 525°F