Polymer Name: PC/ASA Alloy

Processing Methods: Injection Molding

Density: 1150.0 - 1150.0 kg/m³

Flexural Modulus: 186.0 - 186.0 MPa

Technical Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Polymer Name
Plastics & Elastomers Functions
Technologies

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Strength at Yield48MPaASTM D 638
Tensile Elongation at Break20%ISO 527
Tensile Modulus1862MPaASTM D 638
Flexural Strength72MPaASTM D 790
Flexural Modulus186MPaASTM D 790
Izod Notched Impact Strength (73°F)801J/mASTM D256
Physical Properties
ValueUnitsTest Method / Conditions
Melt Flow Rate - MFR (260°C/5.0 kg)14g/10minASTM D1238
Molding Shrinkage - Cross Flow0.005%ASTM D955
Molding Shrinkage - Flow (0.126 in (3.20 mm))0.005 - 0.009mm/mmASTM D955
Specific Gravity1.15-ASTM D 792
Water Absorption0.1%ASTM D570
Thermal Properties
ValueUnitsTest Method / Conditions
Heat Deflection Temperature - HDT (264 psi)110°CASTM D648
Heat Deflection Temperature - HDT (66 psi)121°CASTM D648
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Drying Temperature212°F
Drying Time2hr
Maximum Drying Time6h
Suggested Maximum Moisture0.0002%
Suggested Shot Size45 - 80%
Rear Barrel Temperature450 - 480°F
Middle Barrel Temperatures450 - 480°F
Front Barrel Temperatures460 - 490°F
Nozzle Temperature460 - 500°F
Back Pressure25 - 95psi
Mold Temperature130 - 160°F
Screw Speed25 - 80rpm
Melt Temperature500 - 530°F