EnVoy™ 2506UR

1 of 3 products in this brand

Polymer Name: Acrylonitrile Styrene Acrylate (ASA)

Processing Methods: Injection Molding

Melt Flow Index: 22.0 - 22.0 g/10 min

Technical Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Chemical Family
Plastics & Elastomers Functions
Technologies

Features & Benefits

Applications & Uses

Plastics & Elastomers Processing Methods

Properties

Flame Rating
Flame Rating
UL 94 HB
Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Strength at Yield41MPaASTM D 638
Tensile Elongation at Break25%ASTM D638
Flexural Strength69MPaASTM D790
Flexural Modulus2414MPaASTM D 790
Izod Notched Impact Strength (73°F)481J/mASTM D256
Physical Properties
ValueUnitsTest Method / Conditions
Melt Flow Rate - MFR (260°C/3.8 kg)22g/10minASTM D1238
Molding Shrinkage - Flow (0.126 in (3.20 mm))0.127 - 0.229mm/mmASTM D955
Specific Gravity1.17-ASTM D 792
Water Absorption0.5%ASTM D570
Thermal Properties
ValueUnitsTest Method / Conditions
Heat Deflection Temperature - HDT (264 psi)105°CASTM D648
Heat Deflection Temperature - HDT (66 psi)100°CASTM D648
Flammability
ValueUnitsTest Method / Conditions
Flame Rating (0.125)HB-UL 94
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Drying Temperature220°F
Drying Time4hr
Maximum Drying Time6h
Suggested Maximum Moisture0.0002%
Suggested Shot Size25 - 75%
Rear Barrel Temperature470 - 510°F
Middle Barrel Temperatures480 - 520°F
Front Barrel Temperatures490 - 530°F
Nozzle Temperature490 - 530°F
Back Pressure25 - 95psi
Mold Temperature900 - 160°F
Screw Speed25 - 80rpm
Melt Temperature500 - 530°F