company tower banner
Felli Company Logo

PlasticWood Compound PP40 SCD

PlasticWood Compound PP40 SCD contains renewable resources.

Polymer Name: Polypropylene (unspecified)

Processing Methods: Injection Molding

    Knowde Enhanced TDS

    Identification & Functionality

    Plastics & Elastomers Functions
    Technologies
    Country of Origin

    Europe

    Features & Benefits

    Materials Features

    Applications & Uses

    Plastics & Elastomers Processing Methods
    Processing Methods

    Injection molding

    Properties

    Physical Properties
    ValueUnitsTest Method / Conditions
    Melt flow rate, MFR29.0cm /10minISO 1133
    Temperature190.0°C-
    Load10.0kg-
    Mechanical Properties
    ValueUnitsTest Method / Conditions
    Tensile modulus1740.0MPaISO 527
    Break voltage32.0MPaISO 527
    Elongation at break5.0%ISO 527
    Flexural modulus (23°C)3490.0MPaISO 178
    Impact strength according to Charpy (23°C)13.0kJ/m2ISO 179 / 1eU
    Typical Properties
    ValueUnitsTest Method / Conditions
    Density1060.0kg/mISO 1183
    Processing Information (Injection Molding)
    ValueUnitsTest Method / Conditions
    Predrying temperature100.0°C-
    Pre-drying time7.0h-
    Processing moisturemax. 0.05%-
    Mold temperature40 - 60°C-
    Zone 1160 - 165°C-
    Nozzle temperature175 - 180°C-

    Packaging & Availability

    Regional Availability
    • Europe