Sparkle 660 is used for the preparation of pearlescent surfactant formulations.
Properties
- Physical Form
- Appearance
- Pearly viscous liquid white
- Odor
- Characteristic
- Microbiological Values
- Specifications
Value | Units | Test Method / Conditions | |
Microbial Count (TVC) | max. 10 | cfu/ml | - |
Microbial Count (Y/M) | max. 10 | cfu/ml | - |
Value | Units | Test Method / Conditions | |
pH (10 % aqueous solution) | 5 - 7 | - | - |
Solids Content (at 105°C, 2 hrs) | 40 - 45 | % by mass | - |
Viscosity (at 30°C, #4, 30 rpm) | max. 10000 | cps | Brookfield LVT |
Packaging & Availability
- Packaging Type
- Packaging Information
Sparkle 660 is available in 220 liter HMHDPE carboys. Total of 80 carboys i.e. 12 MT (150 kg per carboy) can be shipped either palletized or non-palletized in 20 ft. full container load.
Storage & Handling
- Shelf Life
- 1 Year
- Storage & Handling Information
- Store in a clean, dry place. Keep containers tightly closed.
- The recommended storage temperature is 25 - 35°C.
- In the original sealed containers and kept at suggested storage conditions, Sparkle 660 can be stored for at least 1 year.
- Slight separation may occur during storage, which can be reversed by stirring, without affecting the pearlizing property of the product.
- Metal containers are not suitable for storing Sparkle 660, as it may corrode the container.
- Storage tanks made of stainless steel (SS 316) or FRP are suitable for storing this product.
Sparkle 660 should be processed at temperatures 15 - 35°C. Outside this range, the viscosity may increase, making it difficult to pump. This characteristic property can be reversed by stirring the product at 25 - 35°C.