Injection (Super high impact)
Properties
- Flame Rating
- Physical Properties
Value | Units | Test Method / Conditions | |
Flammability | HB (1.5) | - | UL-94 |
Flexural Modulus (23⁰C) | 2.05 | ×104kg/cm2 | ASTM D790 |
Flexural Strength At Yield (23⁰C) | 570.0 | kg/cm2 | ASTM D790 |
Heat Distortion Temperature (1/4", 18.6 Kg/Cm2) | 84.0 | ⁰C | ASTM D648 |
Heat Distortion Temperature (1/4", 4.6 Kg/Cm2) | 90.0 | ⁰C | ASTM D648 |
Izod Notched Impact (1/4", 23⁰C) | 36.0 | Kg-cm/cm | ASTM D256 |
Melt Flow Index (10 Kg/220⁰C) | 17.0 | g/10 min | ASTM D1238 |
R °Ckwell Hardness (1/4", 23⁰C) | 109.0 | R-Scale | ASTM D785 |
Tensile Strength At Yield (23⁰C) | 420.0 | kg/cm2 | ASTM D638 |
Regulatory & Compliance
- Certifications & Compliance
Technical Details & Test Data
- Processing Technique
Drying Temperature: 80-85⁰C, 2-3 hrs
Processing Temperature: 210-260⁰C