KM-Polycarb 2031-50 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.

Polymer Name: Polycarbonate (PC)

Processing Methods: Extrusion, Injection Molding

Additives Included: UV Stabilizer

Flexural Modulus: 2410.0 - 2410.0 MPa

Technical Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Additives Included
Chemical Family
Polymer Name
Technologies

Features & Benefits

Characteristics

• UV stabilizer

Applications & Uses

Plastics & Elastomers End Uses
Plastics & Elastomers Processing Methods
Applications
  • High viscosity
  • 0% UV light transmittance at wavelength below 380 nm
  • Applications
  • Sheet
  • Appliances
  • Optical lens
  • Film

Properties

Physical Properties
ValueUnitsTest Method / Conditions
Melt Flow Rate (300°C, 1.2 kg)5g/10 minASTM D 1238
Density1200kg/m³ASTM D 792
Mold Shrinkage0.005 - 0.007mm/mmASTM D 955
Water Absorption (24 hrs, 23°C)0.15%ASTM D 570
Water Absorption (50%RH, 23°C)0.32%ASTM D 570
Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Yield Strength60MPaASTM D 638
Ultimate Tensile Strength72MPaASTM D 638
Elongation at Yield6%ASTM D 638
Elongation at Break150%ASTM D 638
Tensile Modulus2410MPaASTM D 638
Flexural Strength96MPaASTM D 790
Flexural Modulus2410MPaASTM D 790
Notched lzod Impact (23°C)950J/mASTM D 256
Unnotched Izod Impact (23°C)No breakASTM D 256
Instrumented Dart Impact, Total Energy (23°C)94JASTM D 3763
Rockwell Hardness74M ScaleASTM D 785
Taber Abrasion Resistance (A Haze)45%ASTM D 1044
Thermal Properties
ValueUnitsTest Method / Conditions
Deflection Temperature Under Load (4 mm at 66 psi, Annealed)146°FASTM D 648
Deflection Temperature Under Load (264 psi, Annealed)143°CASTM D 648
Deflection Temperature Under Load (264 psi, Unannealed)132°CASTM D 648
Vicat Softening Point (50°C/hr, 50N Load)151°CASTM D 1525
Coefficient of Linear Thermal Expansion (-40 - 82°C)68 x 10^-6mm/mm/°CASTM D 696
Typical Properties
ValueUnitsTest Method / Conditions
Ignition Resistance (0.5 mm)V-2UL-94ASTM D635
Ignition Resistance (1.6 mm)V-2UL-94ASTM D635
Ignition Resistance (2.5 mm)V-2UL-94ASTM D635
Ignition Resistance (UL-94, 0.5mm)V-2ASTM D635
Ignition Resistance (UL-94, 1.6mm)V-2ASTM D635
Ignition Resistance (UL-94, 2.5mm)V-2ASTM D635
Ignition Resistance (UL-94, 3.0mm)V-2ASTM D635
Limiting Oxygen Index26%ASTM D 2863
Ball Indentation Temperaturemin. 125°CIEC 598-1
Average Extent of Burning25mmASTM D 635
Electrical Properties
ValueUnitsTest Method / Conditions
GWT (2.0 mm, 5 second)850°CIEC 695-2-1
Compression Tracking Index (2.0 mm)250VIEC 112
Dielectric Strength17KV/mmASTM D 149
Dielectric Constant (60 Hz)3HzASTM D 150
Dissipation Factor (60 Hz)0.001ASTM D 150
Volume Resistivity (23°C, Dry)2.0 x 10^17cmASTM D 257
Optical Properties
ValueUnitsTest Method / Conditions
Refractive Index (Nd)1.586ASTM D 542
Light Transmittance89%ASTM D 1003
Haze0.7 - 1.5%ASTM D 1003