company tower banner
Novista Company Logo

Novista Chlorinated Polyethylene CM 130A

Novista Chlorinated Polyethylene CM 130A is one chlorinated polyethylene thermoplastic elastomer, which also has excellent low-temperature toughness and processing ability. The processing property with the high dosage of inorganic filler still keep good and the surface of the production will be smooth and exquisite.

Polymer Name: Chlorinated Polyethylene (CPE)

Features: Good Processability, Good Surface Finish, Low Temperature Toughness

Technical Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Plastics & Elastomers Functions
Technologies

Features & Benefits

Applications & Uses

Compatible Polymers & Resins
Applications

It is used for magnetic rubber production and also used as modifier for non-polar rubber for example EPDM.

130A+ ferric oxide powder+ additives

Manufacture magnetic rubber tape of fridge; magnetic board and various rolling magnetic marker.

130A+EPDM+flame retardant +cross linking agent

Manufacture wire and cable sheath, cross linking modifier EPDM waterproof coiled material.

Properties

Physical Form
Typical Properties
ValueUnitsTest Method / Conditions
Chlorine Content35+1%ISO 7725
Hardnessmax. 65Shore AISO 7619
Heat of Fusionmax. 2J/g/100gDSC
Elongation at Breakmin. 700%ISO 37
Mooney Viscosity65 - 75ML(125°C 1+4)
Whiteness E457min. 80°
Rate of Filtration (#40 mesh)min. 98%
Tensile Strengthmin. 8.0MpaISO 37
Volatile Matter Componentmax. 0.4%ISO 1269

Packaging & Availability

Packaging Type
Packaging and Storage

25kg PP valve bag;
The product can be stored under appropriate conditions for two years. But please keep products store in a dry ventilated environment (temperature should not exceed 30°C, in low
humidity). Inappropriate storage environment may cause agglomeration. Especially at high temperatures & high humidity, it is recommended not to stack more than 30 days long, it
may increase agglomeration phenomenon. Agglomeration does not affect the quality and performance, not a quality problem, but agglomeration material is smashed before using .