Polymer Name: Polypropylene Homopolymer (HPP)

Processing Methods: Injection Molding

Melt Flow Index: 24.0 - 24.0 g/10 min

Technical Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Plastics & Elastomers Functions
Technologies

Features & Benefits

Applications & Uses

Plastics & Elastomers Processing Methods
Applications

Fiber production for textile: BCF, carpets, rugs, furnishing fabricsInjection molding: toys, households

Recommended Processing Conditions

Injection molding applications;

Typical melt temperature: 200 - 260°C

Typical mold temperature: 20 - 40°C

Typical injection pressure: 25 - 55 MPa

Processing conditions should be optimized for different equipment design.

Properties

Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Strength at Yield38MPaASTM D638
Flexural Modulus, 23°C1470MPaTS EN ISO 180
Izod Impact Strength at 23°C (notched)20J/mASTM D2372
Rockwell Hardness96Scale RASTM D2901
Typical Properties
ValueUnitsTest Method / Conditions
Melt Flow Rate (230°C/2.16 kg)24g/12ASTM D1238
Density0.905g/cmASTM D1505
Melting Point (DSC, 2nd heating)163°CASTM D3418
Thermal Properties
ValueUnitsTest Method / Conditions
Heat Deflection Temperature at 0.45 MPa87°CISO 77

Regulatory & Compliance

Certifications & Compliance
Recycling

The product is not hazardous or toxic and it is suitable for recycling using available recycling methods.

Packaging & Availability

Packaging

The material is packaged in PE bags or in PP Big Bags. The product should be stored in a dry area with an ambient temperature below 50°C. It should be kept away from sunlight, sparks, heat and flame.

Storage & Handling

Storage

Inappropriate storage conditions can lead to bad smell, color changes and the deterioration in physical properties. It is advised to process PP resins within 6 months after delivery.