Knowde Enhanced TDS
Identification & Functionality
- Additives Included
- Chemical Family
- Fillers Included
- Polymer Name
- Plastics & Elastomers Functions
- Technologies
- Product Families
Features & Benefits
- Materials Features
- Key Features
Good chemical, physical and electrical properties.
Applications & Uses
- Applications
- Plastics & Elastomers Processing Methods
- Applications
- Injection and extrusion molding
- Excellent mechanical performance
- High productivity
- Great surface appearance
- Good processing at high temperatures
Properties
- Color
- Flame Rating
- Resin ID
- PA66 GF50
- Mechanical Properties
- Physical Properties
- Thermal Properties
- Typical Properties
- Properties
- Fiberglass composites with up to 50% filler.
- Flame propagation resistance: GWT 960°C.
- Development of specific colors with Nylon base.
- Additives for UV protection applications.
Value | Units | Test Method / Conditions | |
Charpy Impact Strength (-30°C, 50% RH) | 95 | kJ/m² | ISO 179/1eU |
Charpy Impact Strength (23°C, 50% RH) | 115 | kJ/m² | ISO 179/1eU |
Charpy Impact Strength (23°C, Dry) | 110 | kJ/m² | ISO 179/1eU |
Charpy Impact Strength (23°C) | 110 | kJ/m² | ISO 179/1eU |
Flexural Modulus | 14000 | MPa | ISO 178 |
Charpy Impact Strength (30°C) | 95 | kJ/m² | ISO 179/1eU |
Charpy Notched Impact Strength (-30°C, 50% RH) | 15 | kJ/m² | ISO 179/1eA |
Charpy Notched Impact Strength (23°C, Dry) | 17 | kJ/m² | ISO 179/1eA |
Co-efficient of Linear Thermal Expansion (Parallel, 23 - 55 °C) | 0.14 | E-4/°C | ASTM E 831 |
Flexural Strength | 314 | MPa | ISO 178 |
Izod Impact Strength (30°C, 50% RH) | 15 | kJ/m² | ISO 180/1U |
Izod Impact Strength (30°C, Dry) | 15 | kJ/m² | ISO 180/1U |
Strain at Break (50% RH) | 3.5 | % | ISO 527-1-2 |
Strain at Break (Dry) | 2.7 | % | ISO 527-1-2 |
Stress at Break (50% RH) | 205 | MPa | ISO 527-1-1 |
Stress at Break (Dry) | 260 | MPa | ISO 527-1-1 |
Tensile Modulus (50% RH) | 12900 | MPa | ISO 527-1-2 |
Tensile Modulus (Dry) | 16800 | MPa | ISO 527-1-2 |
Yeild Stress (50% RH) | 200 | MPa | ISO 527-1-2 |
Yield Strain (50% RH) | 3.4 | % | ISO 527-1-2 |
Value | Units | Test Method / Conditions | |
Co-efficient of Linear Thermal Expansion (Transverse, 23 - 55 °C) | 0.72 | E-4/°C | ASTM E 831 |
Flammability (0.6mm) | HB | — | UL94 |
Value | Units | Test Method / Conditions | |
Melting Point | 250 - 265 | °C | ISO 3146/A |
Charpy Impact Strength (-30°C, Dry) | 95 | kJ/m² | ISO 179/1eU |
Charpy Notched Impact Strength (-30°C, Dry) | 16 | kJ/m² | ISO 179/1eA |
Charpy Notched Impact Strength (23°C, 50% RH) | 19 | kJ/m² | ISO 179/1eA |
Heat Deflection Temperature (0.45MPa) | 262 | °C | ISO 75-1-2 |
Heat Deflection Temperature (1.80MPa) | 257 | °C | ISO 75-1-2 |
Izod Notched Impact Strength (23°C, 50% RH) | 20 | kJ/m² | ISO 180/1A |
Izod Notched Impact Strength (23°C, Dry) | 18 | kJ/m² | ISO 180/1A |
Vicat Softening Temperature (50N, 50°C/h) | 254 | °C | ISO 306 |
Yeild Stress (Dry) | 250 | MPa | ISO 527-1-2 |
Yield Strain (Dry) | 2.5 | % | ISO 527-1-2 |
Value | Units | Test Method / Conditions | |
Density | 1.56 | g/cm³ | ISO 1183 |
Regulatory & Compliance
- Certifications & Compliance