Properties
- Flame Rating
- Flame Rating
- UL 94 HB
- Filler Content
- 48 - 52
- Mechanical Properties
- Physical Properties
- Thermal Properties
- Flammability
Value | Units | Test Method / Conditions | |
Tensile Strength | max. 210.0/150.0 | MPa | ISO 527-2 |
Flexural Strength | max. 290.0/270.0 | MPa | ISO 178 |
Hardness (15 s) | 81 | Shore D | D2240 |
Elongation at Break | 2.0/2.5 | % | ISO 527-2 |
Flexural Modulus (23°C) | 14000.0/12500.0 | MPa | ISO 178 |
Tensile Modulus (23°C) | 16000.0/12700.0 | MPa | ISO 527-2 |
Charpy Unnotched Impact Strength (23°C) | NB | kJ/m² | ISO 179 |
Charpy Notched Impact Strength (-30°C) | 8.5 | kJ/m² | ISO 179 |
Charpy Notched Impact Strength (-20°C) | 12 | kJ/m² | ISO 179 |
Charpy Notched Impact Strength (23°C) | 13.0/16.0 | kJ/m² | ISO 179 |
Value | Units | Test Method / Conditions | |
Molding Shrinkage - Flow | 0.2 | % | ISO 294-4 |
Molding Shrinkage - Across Flow | 0.8 | % | ASTM D955 |
Density | 1.56 | g/cm³ | ISO 1183 |
Value | Units | Test Method / Conditions | |
Heat Distortion Temperature B (120°C/h at 455kPa) | 220 | °C | ISO 75/1 |
Heat Distortion Temperature A (120°C/h at 1820kPa) | 215 | °C | ISO 75/1 |
Vicat Softening Tempurature B (50°C/h at 49,05N) | min. 200 | °C | ISO 306 |
Value | Units | Test Method / Conditions | |
Glow Wire Flammability Index - GWFI (2 mm) | 650 | °C | IEC 60695-2-12 |
UL-94 Flammability (1.6 mm) | HB | - | UL94 |