company tower banner
Polymer Resources Ltd. Company Logo

Polymer Resources Ltd. PRL PC-HM-FR2-(color)-3

Polymer Name: Polycarbonate (PC)

Chemical Family: Polycarbonate (PC)

Reinforcement Material: Glass Fibers

Additives Included: Flame Retardant, UV Stabilizer

Fillers Included: Glass Fiber

Processing Methods: Injection Molding

Technical Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Chemical Family
Fillers Included
Polymer Name
Reinforcement Material
Composite Materials Functions
Plastics & Elastomers Functions
Processing Method

Injection Molding

Additive

UV Stabilizer

Filler and Reinforcement
  • Filler : Glass Fiber
  • Reinforcement : 10% Filler by Weight

Features & Benefits

Features
  • Flame Retardant
  • UV Resistant

Applications & Uses

Plastics & Elastomers End Uses
Composites Processing Methods
Plastics & Elastomers Processing Methods

Properties

Physical Form
Physical Properties
ValueUnitsTest Method / Conditions
Density1.26ASTM D792
Melt Mass Flow Rate (at 300°C, 1.2 kg)8.0 - 16g/10 minASTM D1238
Molding Shrinkage (at 0.125 in, Flow)2.0E-3 to 5.0E-3in/inASTM D955
Specific Gravity1.26ASTM D792
Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Strength (at Yield, 0.125 in)9500psiASTM D638
Tensile Strength (at Break, 0.125 in)8100psiASTM D638
Flexural Modulus (at 0.125 in)490000psiASTM D790
Flexural Strength (at 0.125 in)14900psiASTM D790
Thermal Properties
ValueUnitsTest Method / Conditions
Deflection Temperature Under Load (at 66 psi, 0.125 in, Unannealed)290°FASTM D648
Deflection Temperature Under Load (at 264 psi, 0.125 in, Unannealed)280°FASTM D648
Flammability
ValueUnitsTest Method / Conditions
Flame Rating (at 0.06 in, All)V-0UL 94
Flame Rating (at 0.12 in, All)V-0UL 94
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Drying Temperature245 - 255°F
Drying Time3.0 - 4.0hr
Front Temperature600 - 640°F
Middle Temperature580 - 620°F
Mold Temperature180 - 240°F
Maximum Drying Time8hr
Processing Temperature (Melt)575 - 625°F
Rear Temperature560 - 600°F
Impact Properties
ValueUnitsTest Method / Conditions
Impact Strength (at 73°F, 0.125 in, Notched Izod)2ft·lb/inASTM D256

Regulatory & Compliance

Certifications & Compliance
Quality Standards
Agency Ratings & Compliance

RoHS Compliant

Packaging & Availability

Country Availability
Regional Availability
  • North America
Availability

North America