Knowde Enhanced TDS
Identification & Functionality
- Additives Included
- Chemical Family
- Polymer Name
- Composite Materials Functions
- Plastics & Elastomers Functions
- Technologies
- Product Families
- Processing Method
Injection Molding
- Additive
- Flame Retardant
- Impact Modifier
Features & Benefits
- Materials Features
- Features
- Chemical Resistant
- Flame Retardant
- Good Weather Resistance
- Impact Modified
- Low Temperature Impact Resistance
- Self Extinguishing
- Ultra High Impact Resistance
Applications & Uses
- Applications
- Plastics & Elastomers End Uses
- Composites Processing Methods
- Plastics & Elastomers Processing Methods
Properties
- Physical Properties
- Mechanical Properties
- Thermal Properties
- Flammability
- Processing Information (Injection Molding)
- Impact Properties
Value | Units | Test Method / Conditions | |
Density | 1.25 | — | ASTM D792 |
Melt Mass Flow Rate (at 265°C, 2.16 kg) | 5.0 - 12 | g/10 min | ASTM D1238 |
Molding Shrinkage (Flow) | 6.0E-3 to 9.0E-3 | in/in | ASTM D955 |
Specific Gravity | 1.25 | — | ASTM D792 |
Value | Units | Test Method / Conditions | |
Tensile Strength (at Yield, 0.125 in) | 7300 | psi | ASTM D638 |
Tensile Strength (at Break, 0.125 in) | 7000 | psi | ASTM D638 |
Flexural Modulus (at 0.125 in) | 290000 | psi | ASTM D790 |
Flexural Strength (at 0.125 in) | 11000 | psi | ASTM D790 |
Value | Units | Test Method / Conditions | |
Deflection Temperature Under Load (at 66 psi, 0.125 in, Unannealed) | 195 | °F | ASTM D648 |
Deflection Temperature Under Load (at 264 psi, 0.125 in, Unannealed) | 180 | °F | ASTM D648 |
Relative Thermal Index Electrical Property (at 0.06 in) | 167 | °F | UL 746 |
Relative Thermal Index Impact Property (at 0.06 in) | 167 | °F | UL 746 |
Relative Thermal Index Strength Property (at 0.06 in) | 167 | °F | UL 746 |
Value | Units | Test Method / Conditions | |
Flame Rating (at 0.06 in) | V-0 | — | UL 94 |
Value | Units | Test Method / Conditions | |
Drying Temperature | 220 - 230 | °F | — |
Drying Time | 4.0 - 6.0 | hr | — |
Front Temperature | 500 - 540 | °F | — |
Middle Temperature | 490 - 530 | °F | — |
Mold Temperature | 150 - 190 | °F | — |
Rear Temperature | 480 - 520 | °F | — |
Maximum Drying Time | 8 | hr | — |
Processing Temperature (Melt) | 475 - 525 | °F | — |
Value | Units | Test Method / Conditions | |
Impact Strength (at -40°F, 0.125 in, Notched Izod) | 7 | ft·lb/in | ASTM D256 |
Impact Strength (at 73°F, 0.125 in, Notched Izod) | 13 | ft·lb/in | ASTM D256 |
Gardner Impact Strength (at 0.125 in) | 320 | in·lb | ASTM D3029 |
Regulatory & Compliance
- Certifications & Compliance
- Quality Standards
- Agency Ratings & Compliance
RoHS Compliant
Packaging & Availability
- Regional Availability
- Availability
North America