company tower banner
Polymer Resources Ltd. Company Logo

Polymer Resources Ltd. PRL PPX-G20

Polymer Name: PPO/PS Alloy

Chemical Family: Styrenics

Reinforcement Material: Glass Fibers

Processing Methods: Injection Molding

Density: 1200.0 - 1200.0 kg/m³

Technical Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Chemical Family
Fillers Included
Polymer Name
Reinforcement Material
Composite Materials Functions
Plastics & Elastomers Functions
Processing Method

Injection Molding

Filler and Reinforcement
  • Filler : Glass Fiber
  • Reinforcement : 20% Filler by Weight

Features & Benefits

Features
  • Hydrolytically Stable
  • Low to No Water Absorption
  • Medium Heat Resistance

Applications & Uses

Plastics & Elastomers End Uses
Composites Processing Methods
Plastics & Elastomers Processing Methods

Properties

Physical Form
Physical Properties
ValueUnitsTest Method / Conditions
Density1.2ASTM D792
Melt Mass Flow Rate (at 250°C, 11.6 kg)1.0 - 8.0g/10 minASTM D1238
Molding Shrinkage (at 0.125 in, Flow)2.0E-3 to 5.0E-3in/inASTM D955
Specific Gravity1.2ASTM D792
Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Strength (at Yield, 0.125 in)13500psiASTM D638
Tensile Strength (at Break, 0.125 in)13500psiASTM D638
Tensile Elongation (at Break, 0.125 in)3%ASTM D638
Flexural Modulus (at 0.125 in)750000psiASTM D790
Flexural Strength (at 0.125 in)20000psiASTM D790
Thermal Properties
ValueUnitsTest Method / Conditions
Deflection Temperature Under Load (at 66 psi, 0.125 in, Unannealed)280°FASTM D648
Deflection Temperature Under Load (at 264 psi, 0.125 in, Unannealed)270°FASTM D648
Vicat Softening Temperature290°FASTM D1525 ²
Electrical Properties
ValueUnitsTest Method / Conditions
Volume Resistivity10000000000000000ohms·cmASTM D257
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Drying Temperature220 - 230°F
Drying Time3.0 - 4.0hr
Front Temperature540 - 600°F
Middle Temperature520 - 590°F
Mold Temperature160 - 220°F
Rear Temperature500 - 580°F
Maximum Drying Time8hr
Processing Temperature (Melt)550 - 600°F
Impact Properties
ValueUnitsTest Method / Conditions
Impact Strength (at 73°F, Notched Charpy)3ft·lb/in²ISO 179/1
Impact Strength (at -22°F, 0.125 in, Notched Izod)1ft·lb/inASTM D256
Impact Strength (at 73°F, 0.125 in, Notched Izod)1.5ft·lb/inASTM D256
Impact Strength (at 73°F, Notched Izod)3ft·lb/in²ISO 180/1A
Hardness
ValueUnitsTest Method / Conditions
Rockwell Hardness (L-Scale)106ASTM D785

Regulatory & Compliance

Certifications & Compliance
Agency Ratings & Compliance

RoHS Compliant

Packaging & Availability

Country Availability
Regional Availability
  • North America
Availability

North America