Polymer Resources Ltd. PRL TP-FR-G30

Polymer Name: Polybutylene Terephthalate (PBT)

Processing Methods: Injection Molding

Fillers Included: Glass Fiber

Additives Included: Flame Retardant

Technical Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Additives Included
Chemical Family
Fillers Included
Plastics & Elastomers Functions
Technologies
Processing Method

Injection Molding

Additive

Flame Retardant

Filler and Reinforcement
  • Filler : Glass Fiber
  • Reinforcement : 30% Filler by Weight

Features & Benefits

Features
  • Flame Retardant
  • High Heat Resistance
  • Self Extinguishing

Applications & Uses

Plastics & Elastomers End Uses
Plastics & Elastomers Processing Methods

Properties

Physical Form
Physical Properties
ValueUnitsTest Method / Conditions
Density1.62ASTM D792
Melt Mass Flow Rate (at 250°C, 2.16 kg)9.0 - 20g/10 minASTM D1238
Molding Shrinkage (at 0.125 in, Flow)4.0E-3 to 8.0E-3in/inASTM D955
Specific Gravity1.62ASTM D792
Mechanical Properties
ValueUnitsTest Method / Conditions
Tensile Strength (at Yield, 0.125 in)17500psiASTM D638
Tensile Strength (at Break, 0.125 in)17500psiASTM D638
Flexural Modulus (at 0.125 in)1400000psiASTM D790
Flexural Strength (at Break, 0.125 in)27000psiASTM D790
Thermal Properties
ValueUnitsTest Method / Conditions
Deflection Temperature Under Load (at 66 psi, 0.125 in, Unannealed)410°FASTM D648
Deflection Temperature Under Load (at 264 psi, 0.125 in, Unannealed)390°FASTM D648
Relative Thermal Index Electrical Property (at 0.03 in)284°FUL 746
Relative Thermal Index Electrical Property (at 0.06 in)284°FUL 746
Relative Thermal Index Electrical Property (at 0.09 in)284°FUL 746
Relative Thermal Index Electrical Property (at 0.12 in)284°FUL 746
Relative Thermal Index Impact Property (at 0.03 in)266°FUL 746
Relative Thermal Index Impact Property (at 0.06 in)266°FUL 746
Relative Thermal Index Impact Property (at 0.09 in)266°FUL 746
Relative Thermal Index Impact Property (at 0.12 in)266°FUL 746
Relative Thermal Index Strength Property (at 0.03 in)284°FUL 746
Relative Thermal Index Strength Property (at 0.06 in)284°FUL 746
Relative Thermal Index Strength Property (at 0.09 in)284°FUL 746
Relative Thermal Index Strength Property (at 0.12 in)284°FUL 746
Electrical Properties
ValueUnitsTest Method / Conditions
Volume Resistivity10000000000000000ohms·cmASTM D257
Dielectric Strength (at 0.0335 in)580V/milASTM D149
Arc Resistance (at 0.0315 in)PLC 6ASTM D495
Comparative Tracking Index (at 0.0335 in)PLC 2UL 746
High Amp Arc Ignition (at 0.03 in)PLC 0UL 746
High Amp Arc Ignition (at 0.06 in)PLC 0UL 746
High Amp Arc Ignition (at 0.09 in)PLC 0UL 746
High Amp Arc Ignition (at 0.12 in)PLC 0UL 746
High Voltage Arc Tracking Rate (at 0.0335 in)PLC 0UL 746
Hot Wire Ignition (at 0.03 in)PLC 3UL 746
Hot Wire Ignition (at 0.06 in)PLC 2UL 746
Hot Wire Ignition (at 0.09 in)PLC 2UL 746
Hot Wire Ignition (at 0.12 in)PLC 1UL 746
Flammability
ValueUnitsTest Method / Conditions
Flame Rating (at 0.03 in)V-0UL 94
Flame Rating (at 0.06 in)V-0UL 94
Flame Rating (at 0.09 in)V-0, 5VAUL 94
Flame Rating (at 0.12 in)V-0, 5VAUL 94
Processing Information (Injection Molding)
ValueUnitsTest Method / Conditions
Drying Temperature240 - 250°F
Drying Time3.0 - 4.0hr
Front Temperature480 - 510°F
Middle Temperature470 - 500°F
Mold Temperature160 - 190°F
Rear Temperature460 - 490°F
Maximum Drying Time8hr
Processing Temperature (Melt)450 - 500°F
Impact Properties
ValueUnitsTest Method / Conditions
Impact Strength (at 73°F, 0.125 in, Notched Izod)1.2ft·lb/inASTM D256

Regulatory & Compliance

Certifications & Compliance
Quality Standards
Agency Ratings & Compliance

RoHS Compliant

Packaging & Availability

Country Availability
Regional Availability
  • North America
Availability

North America