Polymer Name: Polyester (unspecified)

Chemical Family: Polyesters, Unsaturated Polyester (UPE)

Processing Methods: Continuous Lamination

End Uses: Pipes, Structural Components, Tanks

Technical Data Sheet

Similar Products

  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Composite Materials Functions

Features & Benefits

Materials Features
Product Highlights
  • Low styrene emission
  • Preaccelerated
  • Thixotropic
  • Very good chemical resistance

Applications & Uses

Composites Processing Methods

Properties

Typical Properties
ValueUnitsTest Method / Conditions
Solid Content58 - 62%MT-CU001C
Specific weight at 20°C1,12g/cm3
Brookfield Viscosity at 25°C, sp 3 rpm 50800 - 1000mPa.sMT-CUT25V
Gel Time at 60°C + peroxydes20 - 30minutesMT-CU149R
Curing Time at 60°C + peroxydes23 - 35minutesMT-CU149R
Exothermic peak at 60°C + peroxydes180 - 220°CMT-CU149R
Cured Properties
ValueUnitsTest Method / Conditions
Tensile strength at 40°C for 16h /+ 2 h at 90°C70MPaISO 527 (2012)
Elongation at break at 40°C for 16h /+ 2 h at 90°C3,6%ISO 527 (2012)
Tensile Modulus at 40°C for 16h /+ 2 h at 90°C3500MPaISO 527 (2012)
Flexural strength at 40°C for 16h /+ 2 h at 90°C130MPaISO 178 (2011)
Flexural modulus at 40°C for 16h /+ 2 h at 90°C3500MPaISO 178 (2011)
HDT at 40°C for 16h /+ 2 h at 90°C100°CISO 75 -2A (2013)

Safety & Health

Product Safety

Stir the resin before use, without use air bubbles, As the resin includes a film-forming agent, we recommend that the laminate should first rubbed down before bonding or relaminating.

Storage & Handling

Shelf Life
6 Months (23°C in Dark )