Waterproof Sunscreen with PERMETHYL 284C
Formulation
Name | Ingredient | Supplier | % |
---|---|---|---|
Phase A | |||
Cutina HR Hydrogenated Castor Oil | Hydrogenated Castor Oil | 1 | 1.50 |
Emulsynt 1055 Polyglyceryl-4 Oleate (and) PEG-8 Propylene Glycol Cocoate | Polyglyceryl-4 Oleate (and) PEG-8 Propylene Glycol Cocoate | 2 | 3.50 |
Eutanol G Octyldodecanol | Octyldodecanol | 2 | 2.25 |
Permethyl 284C Polyisobutene and Mixed Alkanes | Polyisobutene and Mixed Alkanes | 3 | 0.50 |
Dow Corning 200/50 cs Fluid Dimethicone | Dimethicone | 4 | 1.00 |
Petrolatum Petrolatum | Petrolatum | 5 | 4.00 |
Ritachol Mineral Oil (and) Lanolin Alcohol | Mineral Oil (and) Lanolin Alcohol | 6 | 1.00 |
Propylparaben Propylparaben | Propylparaben | 2 | 0.10 |
Parsol MCX Ethylmethyl Methoxycinamate | Ethylmethyl Methoxycinamate | 7 | 5.00 |
Crill 6 Sorbitan Isostearate | Sorbitan Isostearate | 8 | 0.50 |
Liponate IPP Isopropyl Palmitate | Isopropyl Palmitate | 9 | 4.50 |
Phase B | |||
Deionised Water Deionised Water | Deionised Water | — | 73.45 |
Methylparaben Methylparaben | Methylparaben | 2 | 0.20 |
Glycerin Glycerin | Glycerin | 1 | 2.00 |
Magnesium Sulfate Magnesium Sulfate | Magnesium Sulfate | — | 0.50 |
Preparation:
Procedure
In a main vessel, mix ingredients in Phase A and heat to 75°C.
Combine Phase B and heat the batch to 80°C. Mix Well.
When Phase A and B are at the appropriate temperatures, add Phase B to
Phase A by homogenising. Homogenise until the batch is smooth and
uniform.
Switch to sweep mixing and cool to 25°C and fill into a appropriate
containers.
Notes:
Suppliers
1 Cognis
2 ISP
3 Presperse Inc.