Enhanced TDS
Knowde-enriched technical product data sheet
Identification & Functionality
- Chemical Family
- Fillers Included
- Polymer Name
- Plastics & Elastomers Functions
- Technologies
- Product Families
- Availability
- Asia Pacific
- Europe
- Latin America
- North America
Features & Benefits
- Materials Features
- Features
- Chemically Coupled
- High Impact Resistance
- High Rigidity
- Homopolymer
Applications & Uses
- Markets
- Plastics & Elastomers Processing Methods
- Processing Method
Injection Molding
Properties
- Color
- Flame Rating
- Appearance
- Natural Color
- Physical Properties
- Mechanical Properties
- Typical Properties
- Thermal Properties
- Flammability
- Processing Information (Injection Molding)
Value | Units | Test Method / Conditions | |
Density at 23°C | 1.15 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 5 | g/10 min | SO 1133 |
Across Flow | 1 | % | - |
Flow | 0.35 | % | - |
Ash Content | 32 | % | ISO 3451 |
Value | Units | Test Method / Conditions | |
Tensile Modulus at 23°C | 7800 | MPa | ISO 527-2/1 |
Tensile Stress Break at 23°C | 97 | MPa | ISO 527-2/50 |
Tensile Strain Break at 23°C | 2.8 | % | ISO 527-2/50 |
Flexural Modulus 2 (23°C) | 7400 | MPa | ISO 178 |
Flexural Stress 3 (23°C) | 150 | MPa | ISO 178 |
Value | Units | Test Method / Conditions | |
Forms | Granules | - | - |
Charpy Unnotched Impact Strength (23°C) | 45 | kJ/m² | ISO 179/1eU |
Notched Izod Impact Strength (23°C) | 9.5 | kJ/m² | ISO 180/1A |
Hardness (15 sec) | 82 | Shore D | ISO 868 |
Value | Units | Test Method / Conditions | |
Heat Deflection Temperature (0.45 MPa, Unannealed) | 163 | °C | ISO 75-2/Bf |
Heat Deflection Temperature (1.8 MPa, Unannealed) | 153 | °C | ISO 75-2/Af |
Vicat Softening Temperature | 137 | °C | ISO 306/B50 |
Accelerated Oven Ageing at 150°C | 1000 | hr | ISO 4577 |
Value | Units | Test Method / Conditions | |
Flame Rating (1.6 mm) | HB | - | UL 97 |
Value | Units | Test Method / Conditions | |
Drying Temperature | 80 to 90 | °C | - |
Drying Time | 2 | hr | - |
Processing (Melt) Temp | 190 to 210 | °C | - |
Mold Temperature | 60 to 70 | °C | - |
Regulatory & Compliance
- Certifications & Compliance
Technical Details & Test Data
- Filler / Reinforcement
Glass Fiber, 30% Filler by Weight