company tower banner
Teca-Print Company Logo

Teca-Print TPC 230

TPC 230 is a pad printing ink with maximum resistance. Best adhesion characteristics with thermoplastics, varnished surfaces, metals, NE-metals, polyamide PA, polycarbonate PC, polyester, polymethacrylate PMMA, polyurethane PUR and hard PVC. Used for industrial and advertising applications.

Compatible Substrates & Surfaces: Iron, Metal, Plastics, Poly(Methyl Methacrylate) (PMMA), Polyamide, Polycarbonate (PC), Polyesters, Polyurethane, Polyvinyl Chloride (PVC), Steel

Features: Abrasion Resistant, Acid Resistant, Alkali Resistant, Chemical Resistant, Excellent Opacity, High Gloss

Application Method: Pad Printing

Technical Data Sheet
  • TypeDocument Name
View All Documents

Knowde Enhanced TDS

Identification & Functionality

Features & Benefits

Properties
  • Quick drying and glossy.
  • High chemical resistance against organic solvent, chemicals, thinned alkalis and acids.
  • The resistance against mechanical abrasion is substantially better compared to TPC 200.
  • Good opacity (excellent in HD).

Applications & Uses

Application Method
Use of Additives
  • Hardener must be used in an appropriate ratio to the ink. Strong deviations from the noted ratios above can lead to problems. Some problems may take a while to show and can eventually affect resistance and adhesion. Thus, after adding hardener and then thinner – this order is very important – the mixture should rest for approx. 15 minutes so that optimum ink flow and adhesion are achieved.
  • Hardener only to increase the chemical resistance.
  • Pot life can be reduced by approx. half for metal color tones. With some ink types, pot life depends on a direct relationship to roomtemperature (RT) and relative air humidity (RAH).
  • Evaporation rate: the lower the value, the faster the evaporation, f = relative evaporation rate compared to VC and VD.
  • Thinner VP increases ink adhesion onto polystyrol and related materials.
  • Extremely mild thinner to protect PMMA and polystyrene (molded pieces) from stress or tension cracks. The thinner VX does not etch into the surface and as a result can also be used as a cleaner.
  • Thinner VR contains XYLOL and cannot be classified as non-hazardous like the other solvents. The flash point is < 0°, extra care is to be taken due to flammability.
  • Adhesion promoter MT is not to be added to the ink. Pre-treatment e.g. via wiping objects with an MT-soaked cloth, spraying or dipping them. Bonding additive MD is a printable “in line” variation of the MT bonding additive and is applied as a single hit prior to the ink application.
  • Bonding additive MT should be added in 10 – 20 % quantities. It does not alter pot life, but does reduce resistance values.
  • General additives can be used for all ink types except for oven cured inks, UV inks and TPC 301.
  • Retarder agents are used for more specialized applications in which a defined thinner-retarder ratio is used.

Properties

Adhesion Properties
SUBSTRATE

Ink ref. System Special

TPC 230
POLYOLEFINES pretreat pre-treated polyethylene PE ++
pre-treated polypropylene PP ++
THERMOPLASTICS polystyrene PS / SB ++
styrene ABS ++
SAN ++
linear polyester PET ++
PET-A, E, P ++
PET-G ++
polyvinylchloride hard PVC ++
soft PVC  
polyacrylate compounds PAN  
polymethylmethacrylate PMMA ++
polymethylacrylate comp. AMMA,MBS ++
polybutylentherphtalate PBTP  
pre-treated polyester   ++
polycarbonate PC ++
polyamide (Nylon) PA ++
polyurethane PUR ++
cellulose acetate CA  
cellulose acetobutyrate CAB +++
POLYOXIDES postflame polyacetal (post treatment!) POM  
POM-C  
THERMOSETS all thermosets spez, auf IC ++
phenoplasts MPF/PPO ++
epoxy resin   ++
aminoplasts   ++
FE-METALS (degrease) stainless steel V2A, V4A  
steel / iron Fe +
NON-FERROUS METALS (degrease) Al, oxidized & brushed AI ++
plated chrome Cr +
copper Cu +
brass brass +
plated nickel Ni +
plated tin Sn +
plated zinc Zn  
LACQUERED SURFACES 1-component lacquer ++
2-comp + UV-powder lacquer +
OTHER MATERIALS glass, ceramics (part. enameled)  
uncoated wood  
paper / cardboard  
leather / synthetic leather  
Elastomerrs untreated rubber  
thermoplastic elastomers  

 

+ = good, ++ = very good, +++ = excellent
(++) = suitable: for increased requirements for chemical resistance, or weatherproof, drying or other special ink characteristics, tests should be conducted. 1 = pre-treated FG = with fiber glass * = oven cured  part. = partially

Packaging & Availability

Ink Ordering Information

Most inks are available in practical 200 ml tubes. Fluorescent tones (TPC 180) are only available in 1 l cans. Delivery timet akes about 4 weeks. The inks types TPC 118, 508 and 528 are available in 500 gram cans. Delivery time takes about 1 week. Metall color inks are only available on demand.

DESCRIPTION ORDER Number DELIVERY
INKS 200 ml- Tube 11/1kg- Can  
TPC 230 F23 ox8xox 2 F23 xx8xox4 from stock